Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 7000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 5000 - 7000 cP
5000 - 7000 cP
Huntsman Araldite GY 281 Bisphenol F Epoxy Resin
Weight per Epoxide (EEW, g/eq) 159 to 172. Max color is 4.Comments/Applications: Unmodified, low viscosity bis F epoxy, good flexibility. FDA listed. Used in coatings, adhesives, tank linings, fl..
Viscosity 3000 - 7000 cP
3000 - 7000 cP
Huntsman AroCy XU 71787.02 L Cyanate Ester
Comments/Applications: Dicyclopentadiene based cyanate ester. Outstanding electrical properties. Low outgassing and equilibrium moisture absorption.Data provided by Ciba Specialty Chemicals.Ciba S..
Viscosity 1500 - 7000 cP
1500 - 7000 cP
Lord Adhesives 5 Mix-In Accelerator for 200, 400, 500 Series
Lord Adhesives 5 Mix-In Accelerator for 200, 400, 500 SeriesLord Accelerator 5 is a mix-in accelerator for Lord 200, 400, and 500 series acrylic adhesives. Use at 20:1 ratio.
Viscosity 3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2030812D3 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 60/40. Applications in medical diagnostics, environmentalScreen Printing Equipment: semi-automatic, manualScreen Types: polye..
Viscosity 3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2040308D2 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 40/60. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
Viscosity 3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2051014P10 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. Applications in medical diagnostics, environmentalScreen Printing Equipment: semi-automatic, manualScreen Types: polye..
Viscosity 3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2080110D2 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. This is has been designed for fine line printing.Screen Printing Equipment: semi-automatic, manualScreen Types: polye..
Viscosity 3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2080409D2 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 85/15. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
Viscosity 3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3500 - 7000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2090225D7 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
Viscosity 3000 - 7000 cP
3000 - 7000 cP
RP-17619
Solvay MIRACARE® MP-24 Surfactant
Description: MIRACARE MP-24 is a universal Performance Concentrate formulated to produce shampoo, skin cleansing, and related bath and toiletry products. With simple water dilution MIRACARE MP-24 yi..
Viscosity 6000 - 7000 cP

@Temperature 23.0 °C
6000 - 7000 cP

@Temperature 73.4 °F
Master Bond EP41S-1 Chemically Resistant Two Component Epoxy System
Master Bond Polymer System EP41S-1 is a two component epoxy resin system designed for durable, high performance bonding, sealing, coating and encapsulating. It successfully withstands prolonged imm..
Viscosity 4000 - 7000 cP

@Temperature 23.0 °C
4000 - 7000 cP

@Temperature 73.4 °F
50 rpm
Epoxy Technology EPO-TEK® 353ND-T5 High Temperature Thixotropic Epoxy
Product Description: EPO-TEK® 353ND-T5 is an intermediate viscosity version of EPO-TEK® 353ND and EPO-TEK® 353ND-T. It was designed for high temperature applications in fiber optics, electronics ..
Viscosity 4000 - 7000 cP

@Temperature 23.0 °C
4000 - 7000 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® OE138 Two Component Epoxy
Material Description: A two component epoxy with intermediate viscosity range between EPO-TEK® 353ND and EPO-TEK® 353ND-T. It is designed for semiconductor glob top applications, as well as use in..
Viscosity 5000 - 7000 cP

@Temperature 23.0 °C
5000 - 7000 cP

@Temperature 73.4 °F
50 rpm
Epoxy Technology EPO-TEK® T7139 Glob Top Epoxy
Product Description: EPO-TEK® T7139 is a two component, electrically insulating, encapsulating epoxy designed for semiconductor glob top applications and package assembly.Advantages & Application N..
Viscosity 6000 - 7000 cP
6000 - 7000 cP
Epoxyset Epoxibond EB-115 Unfilled Epoxy Adhesive
A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc...
Viscosity 4000 - 7000 cP
4000 - 7000 cP
Epoxyset Epoxibond EB-135 Unfilled Epoxy Adhesive
A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-135 has excellent bond strength to various substrat..
Viscosity 6000 - 7000 cP

@Temperature 35.0 °C
6000 - 7000 cP

@Temperature 95.0 °F
C.O.I.M. DIEXTER® G181 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Viscosity 5000 - 7000 cP
5000 - 7000 cP
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating
This phosphate-bonded, alumina coating system bonds exceptionally well to dense refractory ceramics, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C)
Copyright © lookpolymers.com All Rights Reserved