Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 750 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 650 - 750 cP
650 - 750 cP
Liquid State
Palm Labs Adhesives TURBO FUSE SERIES 155-HT (700 cp HIGH TEMPERATURE) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190-HT advanced formula is designed to polymerize instantly by absorbing surface moisture and is recommended for..
Viscosity 4.0 - 750 cP
4.0 - 750 cP
Kazanorgsintez NMPE-1 Low-Molecular Polyethylene
Low-molecular polyethylene of high pressure polyethylene production. Application: Designed for use in the rubber industry, building industry, and other fields. Can also be used as component parts..
Viscosity 100 - 750 cP

@Temperature 190 °C
100 - 750 cP

@Temperature 374 °F
542-111
Westlake Epolene® E-43P Oxidized Low Molecular Weight Polyethylene Polymer
Description: Epolene E-43P is a maleic anhydride grafted polypropylene powder recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul..
Viscosity 550 - 750 cP
550 - 750 cP
Dow CYRACURE™ UVR-6128 Cycloaliphatic Epoxide
CYRACURE™ UVR-6107 cycloaliphatic epoxide is a standard flexibilizing cycloaliphatic epoxide resin. Typical applications include: Metal decoration coatings Overprint varnishes Flexible packaging ..
Viscosity 650 - 750 cP

@Temperature 30.0 °C
650 - 750 cP

@Temperature 86.0 °F
3D Systems Accura® Xtreme White 200 Plastic
Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl..
Viscosity 250 - 750 cP
250 - 750 cP
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Viscosity 500 - 750 cP
500 - 750 cP
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone
Low viscosity, green coating for power resistors to 1100°F (593°C)
Viscosity 550 - 750 cP
550 - 750 cP
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester
Viscosity 200 - 750 cP
200 - 750 cP
#2 SP @ 30 rpm; RP-0596
Solvay RHODOLINE® 646 Surfactant
Description: Highly effective mineral oil defoamer for latex processing.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 646 may be post-added to a latex or coat..