Polymer Property : Viscosity = 750000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 750000 - 3.75e+6 cP
750000 - 3.75e+6 cP
Ritelok GM18 Aluminum Parts Gasket Maker
Anaerobic. Flexible gasket maker for aluminum flanges. Replaces pre-cut gaskets, Does not shrink or relax, flexible, Withstands temperatures from 65°F to 300°F (55°C)-150°C), ..
Viscosity 750000 cP
750000 cP
Before Sintering
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative
NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package..
Viscosity 750000 cP
750000 cP
RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy
EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi..
Viscosity 750000 cP
750000 cP
RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy
Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated tem..
Viscosity 750000 cP
750000 cP
A
Shin-Etsu Silicones LIMSâ„¢ KEG2002-50A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity 750000 cP
750000 cP
B
Shin-Etsu Silicones LIMSâ„¢ KEG2002-50A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity 750000 cP
750000 cP
A
Shin-Etsu Silicones LIMSâ„¢ KE1950-70A/B Elastomer
KE-1950-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy ..
Viscosity 750000 cP
750000 cP
B
Shin-Etsu Silicones LIMSâ„¢ KE1950-70A/B Elastomer
KE-1950-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy ..
Viscosity 750000 cP

@Temperature 160 °C
750000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® 8E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 750000 cP

@Shear Rate 100 1/s,
Temperature 175 °C
750000 cP

@Shear Rate 100 1/s,
Temperature 347 °F
Dow Method
Dow XU 32019.10 Barrier Polymer
Excellent oxygen and water vapor barrier Information provided by Dow
Viscosity 750000 cP
750000 cP
Mixed; TM R050-12
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive
Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..