| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 8.0 cP | 8.0 cP | |
|
Lord Adhesives AP-134 Reactive Polymer Primer or Adhesive for Polar Substrates
Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa..
|
|||
| Viscosity |
8.0
cP @Temperature 25.0 °C |
8.0
cP @Temperature 77.0 °F |
|
|
LyondellBasell TPNB Tripropylene glycol normal butyl ether
Information provided by Lyondell.
|
|||
| Viscosity | 8.0 - 25 cP | 8.0 - 25 cP | As Supplied |
|
Heraeus Cleviosâ„¢ PH 500 Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH 500 is an antistatic material based on PEDO..
|
|||
| Viscosity |
8.0
-
10
cP @Temperature 20.0 °C |
8.0
-
10
cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
|
DuPont Elvanol® 51-08 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade
Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late..
|
|||
| Viscosity | 8.0 cP | 8.0 cP | |
|
Dow Corning SYL-OFF® 7210 RELEASE MODIFIER
Syl-Off® 7210 Release Modifier is a 60% active solids, pre-catalysed, release modifier. General purpose release modifier recommeded for use with Syl-Off® Solvent based, platinum catalysed release ..
|
|||
| Viscosity |
8.0
cP @Temperature 15.5 °C |
8.0
cP @Temperature 59.9 °F |
|
|
Dow Hydroxyethyl Acrylate
Hydroxethyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow
|
|||
| Viscosity | <= 8.0 cP | <= 8.0 cP | |
|
3M Scotchgard™ 18 Low Maintenance Floor Finish
Scotchgard Low Maintenance 18 Floor Finish, a high quality water-based co-polymer emulsion, is an economical finish designed to provide exceptional performance for low traffic areas and low frequenc..
|
|||
| Viscosity | <= 8.0 cP | <= 8.0 cP | |
|
3M Scotchgard™ 25 Low Maintenance Floor Finish
Scotchgard Low Maintenance 25 Floor Finish, a high quality water-based co-polymer emulsion, is designed to provide superior performance compared to traditional acrylic floor finishes for low frequen..
|
|||
| Viscosity | <= 8.0 cP | <= 8.0 cP | |
|
3M Scotchgard™ Resilient Floor Protector
Scotchgard Resilient Floor Protector is a high performance protective floor coating for vinyl tile and vinyl sheet flooring that utilizes multiple polymer technologies to produce a hard surface that..
|
|||
| Viscosity | 8.0 - 120 cP | 8.0 - 120 cP | ISO 3104/3105 |
|
3M Scotch-Weld™ PR100 Plastic and Rubber Instant Adhesive
3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates ..
|
|||