Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 800000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 800000 cP

@Shear Rate 250 1/s,
Temperature 230 °C
800000 cP

@Shear Rate 250 1/s,
Temperature 446 °F
Noltex Soarnol® DT2903 Ethylene Vinyl Alcohol Copolymer
Very low ethylene content, high gas barrier for packaging dry products or for use in packaging material used at normal temperature and humidity. Ethylene content 29 mol%. Volatile matter 0.3%.The ..
Viscosity 800000 cP
800000 cP
melt; SABIC Method
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific)
Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region.
Viscosity 800000 cP

@Temperature 420 °C
800000 cP

@Temperature 788 °F
melt; ISO 11443
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant..
Viscosity 800000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
800000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Viscosity 800000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
800000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Viscosity 800000 cP

@Shear Rate 25.0 1/s,
Temperature 320 °C
800000 cP

@Shear Rate 25.0 1/s,
Temperature 608 °F
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade  (discontinued **)
Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui..
Viscosity 800000 cP
800000 cP
B
Shin-Etsu Silicones LIMSâ„¢ KE2090-30AB Elastomer
KE-2090-30 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Viscosity 800000 cP
800000 cP
B
Shin-Etsu Silicones LIMSâ„¢ KE2004-10A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity 800000 cP
800000 cP
B
Shin-Etsu Silicones LIMSâ„¢ KE2090-50AB Elastomer
KE-2090-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Viscosity 800000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
800000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 3101 Acid-/Acrylate-Modified EVA Adhesive Resin
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Viscosity 800000 - 3.75e+6 cP
800000 - 3.75e+6 cP
Thixotropic
Loctite® Gasket Eliminator® 518 Flange Sealant
Anaerobic GasketingLoctite® 518 Flexible Cure Gasket Eliminator® Flange SealantForms a flexible, solvent-resistance seal that will not tear or decay. Seals to 300ºF and fills gaps to 0.050". Can..
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
DSM Akulon® F130 PA6
Film Extrusion, Medium Viscosity
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
DSM Akulon® F132 PA6
Film Extrusion, High Viscosity
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
DSM Akulon® F132-E1 PA6
Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
DSM Akulon® F132-E2 PA6
High Viscosity, Nucleated, Lubricated, Film Extrusion
Viscosity 800000 cP

@Temperature 160 °C
800000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 800000 cP

@Temperature 160 °C
800000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 800000 cP

@Temperature 160 °C
800000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 800000 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
800000 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity
Viscosity 800000 - 1.20e+6 cP
800000 - 1.20e+6 cP
BASF Master Builders Solutions ChemRex® CX-948 Urethane Adhesive/Sealant
Typical applications include high-solids subfloor adhesive, manufacture of windows, doors, and panels, and the assembly of trucks, cabs, and vans.The working open time is 45-60 minutes. The freeze-..
Viscosity 800000 - 1.30e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
800000 - 1.30e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Viscosity 800000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
800000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Advanced Polymer Alloys Alcryn® 1080 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Viscosity 800000 cP
800000 cP
Part A, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
Viscosity 800000 cP
800000 cP
Part A, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive
Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
Viscosity 800000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
800000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 3859 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Copyright © lookpolymers.com All Rights Reserved