Polymer Property : Viscosity = 810000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 810000 cP

@Temperature 260 °C
810000 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F130 PA6
Film Extrusion, Medium Viscosity
Viscosity 810000 cP

@Temperature 260 °C
810000 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F130-C PA6
Film Extrusion, Medium Viscosity, Lubricated
Viscosity 810000 cP

@Temperature 260 °C
810000 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Viscosity 810000 cP

@Temperature 260 °C
810000 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Viscosity 810000 cP

@Temperature 260 °C
810000 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
Viscosity 810000 cP

@Temperature 260 °C
810000 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock
Viscosity 810000 - 2.74e+6 cP

@Temperature 260 - 260 °C
810000 - 2.74e+6 cP

@Temperature 500 - 500 °F
Average value: 1.26e+6 cP Grade Count:6
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..