Polymer Property : Viscosity = 850000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 175000 - 850000 cP

@Temperature 400 - 420 °C
175000 - 850000 cP

@Temperature 752 - 788 °F
Average value: 513000 cP Grade Count:11
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Viscosity 350000 - 850000 cP

@Temperature 400 - 400 °C
350000 - 850000 cP

@Temperature 752 - 752 °F
Average value: 445000 cP Grade Count:3
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Viscosity 350000 - 850000 cP

@Shear Rate 1000 - 1000 1/s
350000 - 850000 cP

@Shear Rate 1000 - 1000 1/s
Average value: 445000 cP Grade Count:3
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..