| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
700
-
900
cP @Temperature 23.0 °C |
700
-
900
cP @Temperature 73.4 °F |
|
|
Prodways PLASTCure Flex 100 3D Printing Polymer
High workability. Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Suitable for the manufacture of flexible objects for..
|
|||
| Viscosity |
500
-
900
cP @Temperature 82.2 °C |
500
-
900
cP @Temperature 180 °F |
|
|
Northstar Polymers MGA-036 Polyether Prepolymer
Information provided by Northstar Polymers.
|
|||
| Viscosity |
600
-
900
cP @Temperature 25.0 °C |
600
-
900
cP @Temperature 77.0 °F |
|
|
Northstar Polymers PLA-012 Polyether Curing Agent
Information provided by Northstar Polymers.
|
|||
| Viscosity |
300
-
900
cP @Temperature 25.0 °C |
300
-
900
cP @Temperature 77.0 °F |
|
|
Northstar Polymers PPA-017 Curing Agent
Information provided by Northstar Polymers.
|
|||
| Viscosity |
300
-
900
cP @Temperature 25.0 °C |
300
-
900
cP @Temperature 77.0 °F |
|
|
Northstar Polymers CPB-046 Polyether Curing Agent
Information provided by Northstar Polymers.
|
|||
| Viscosity | 500 - 900 cP | 500 - 900 cP | |
|
Huntsman HY 955 Polyamide
Approx. H+ equivalent weight 65. Mix Ratio with GY 6010 is 35.Comments/Applications: Modified liquid amidoamine, low viscosity. Adhesives, coatings, flooring, potting and we lay-up applications. ..
|
|||
| Viscosity | 500 - 900 cP | 500 - 900 cP | 15% solids in MEK |
|
Taiwan Sheen Soon Sheenthane® AS-422 TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo..
|
|||
| Viscosity | 600 - 900 cP | 600 - 900 cP | |
|
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 15..
|
|||
| Viscosity | 600 - 900 cP | 600 - 900 cP | |
|
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F.
|
|||
| Viscosity | 600 - 900 cP | 600 - 900 cP | |
|
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F.
|
|||
| Viscosity | 600 - 900 cP | 600 - 900 cP | |
|
Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled
Ceramic-based, black-pigmented coating for carbon and stainless steel to 2000 °F (1093°C).
|
|||
| Viscosity | 400 - 900 cP | 400 - 900 cP | |
|
Aremco Ceramacoat™ 845-SIL High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, matte silver coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..
|
|||
| Viscosity | 250 - 900 cP | 250 - 900 cP | |
|
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F.
|
|||
| Viscosity | 400 - 900 cP | 400 - 900 cP | |
|
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone
Low viscosity, white coating for motor windings to 1100°F (593°C)
|
|||
| Viscosity | 200 - 900 cP | 200 - 900 cP | #2 sp @ 30 rpm; RP-0596 |
|
Solvay RHODOLINE® 679 Surfactant
Description: Highly effective mineral oil defoamer for latex processing.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 679 is recommended for application at 0...
|
|||