| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Saybolt Viscosity at 100°F | 3476 SUS | 3476 SUS | |
|
ChevronTexaco ISO 680 Cylinder Oil W
FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal..
|
|||
| Saybolt Viscosity at 100°F | 3476 SUS | 3476 SUS | |
|
ChevronTexaco Vanguard® 680
Texaco Vanguard oils deliver value through:Excellent metal wettability and high film strength for any moisture condition.Versatility — Three viscosity grades available to cover the range of steam p..
|
|||