| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 1.00 g/10 min | 1.00 g/10 min | |
|
S&E Specialty Polymers TufFill™ GPE3003-36 Natural Flame Retardant concentrate in Polyethylene
Flame Retardant Concentrate in Polyethylene. GPE3003-36 is PE based, flame retardant concentrate, with 1.47 g/cm3 Gravity and Melt Flow of 1.00, designed to impart flame resistance to polyolefin. De..
|
|||
| Melt Flow | 1.00 - 63.0 g/10 min | 1.00 - 63.0 g/10 min | Average value: 19.0 g/10 min Grade Count:110 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
|
|||
| Melt Flow | 1.00 - 120 g/10 min | 1.00 - 120 g/10 min | Average value: 7.88 g/10 min Grade Count:103 |
|
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
|
|||
| Melt Flow | 1.00 - 16.0 g/10 min | 1.00 - 16.0 g/10 min | Average value: 8.07 g/10 min Grade Count:7 |
|
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum ..
|
|||
| Melt Flow | 1.00 - 36.0 g/10 min | 1.00 - 36.0 g/10 min | Average value: 12.2 g/10 min Grade Count:17 |
|
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
|
|||
| Melt Flow | 1.00 - 550 g/10 min | 1.00 - 550 g/10 min | Average value: 31.9 g/10 min Grade Count:22 |
|
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
|
|||
| Melt Flow | 1.00 - 64.2 g/10 min | 1.00 - 64.2 g/10 min | Average value: 15.1 g/10 min Grade Count:38 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
|
|||
| Melt Flow | 1.00 - 78.7 g/10 min | 1.00 - 78.7 g/10 min | Average value: 32.5 g/10 min Grade Count:22 |
|
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
|
|||
| Melt Flow | 1.00 - 2.00 g/10 min | 1.00 - 2.00 g/10 min | Average value: 1.81 g/10 min Grade Count:10 |
|
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Melt Flow | 1.00 - 5.00 g/10 min | 1.00 - 5.00 g/10 min | Average value: 3.00 g/10 min Grade Count:5 |
|
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
|
|||
| Melt Flow |
1.00
g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00
g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
|
Teknor Apex Monprene® MP-1500L2 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
1.00
g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00
g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
|
Teknor Apex Monprene® MP-1504-L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
1.00
g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00
g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
|
Teknor Apex Monprene® MP-1380A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
1.00
g/10 min @Load 2.16 kg, Temperature 230 °C |
1.00
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Teknor Apex Monprene® MP-2465A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
1.00
g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00
g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
|
Teknor Apex Monprene® MP-3004-HH Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
1.00
-
10.0
g/10 min @Load 10.0 kg, Temperature 190 °C |
1.00
-
10.0
g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
|
Teknor Apex Sinpolene MBB3131 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Melt Flow |
>=
1.00
g/10 min @Load 10.0 kg, Temperature 190 °C |
>=
1.00
g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
|
Teknor Apex Sinpolene MBB3331/A Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (350000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Melt Flow |
1.00
g/10 min @Load 2.16 kg, Temperature 230 °C |
1.00
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Teknor Apex Telcar® OBC 2419A Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
|
|||
| Melt Flow |
1.00
g/10 min @Load 2.16 kg, Temperature 230 °C |
1.00
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Teknor Apex Telcar® TL EF-6177B-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Melt Flow |
1.00
g/10 min @Load 2.16 kg, Temperature 230 °C |
1.00
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Teknor Apex Telcar® TL-1654B Thermoplastic Elastomer
Notes: Non-halogenated Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstr..
|
|||
| Melt Flow |
1.00
g/10 min @Load 2.16 kg, Temperature 190 °C |
1.00
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Teknor Apex Telcar® TL-2530F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Melt Flow |
1.00
g/10 min @Load 2.16 kg, Temperature 230 °C |
1.00
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Teknor Apex Telcar® TL-81-D965-P Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Melt Flow |
1.00
g/10 min @Load 2.16 kg, Temperature 230 °C |
1.00
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Teknor Apex Telcar® TL-90-T3030A-80 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
|
|||
| Melt Flow |
1.00
g/10 min @Load 2.16 kg, Temperature 230 °C |
1.00
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Teknor Apex Telcar® TL-91-T3056S-90 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Melt Flow |
1.00
g/10 min @Load 5.00 kg, Temperature 200 °C |
1.00
g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
|
Teknor Apex Monprene® MP-2730 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow | 1.00 - 6.00 g/10 min | 1.00 - 6.00 g/10 min | Average value: 2.90 g/10 min Grade Count:5 |
|
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Sheet/Profile extrusions". Each property range of values reported is mi..
|
|||
| Melt Flow | 1.00 - 101 g/10 min | 1.00 - 101 g/10 min | Average value: 30.6 g/10 min Grade Count:88 |
|
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
|
|||
| Melt Flow | 1.00 - 198 g/10 min | 1.00 - 198 g/10 min | Average value: 59.2 g/10 min Grade Count:59 |
|
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Melt Flow | 1.00 - 15.0 g/10 min | 1.00 - 15.0 g/10 min | Average value: 8.72 g/10 min Grade Count:73 |
|
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
|
|||
| Melt Flow | 1.00 - 280 g/10 min | 1.00 - 280 g/10 min | Average value: 19.3 g/10 min Grade Count:41 |
|
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
|
|||