| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
10.0
g/10 min <br>@Load 4.50 kg,<br> Temperature 260 °C
|
10.0
g/10 min <br>@Load 9.92 lb,<br> Temperature 500 °F
|
ASTM D123 |
|
Niche Polymer PCABSN8BK PC/ABS
Information provided by Niche Polymer
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
10.0
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Teknor Apex Elexar® EL 8732R Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
10.0
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Teknor Apex Monprene® MP-1665-L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 125 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 257 °F
|
ASTM D1238 |
|
Teknor Apex Monprene® MP-1900 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
10.0
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Teknor Apex Monprene® MP-2111 L2 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
10.0
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Teknor Apex Monprene® MP 1257 Thermoplastic Elastomer
Notes: General Purpose; CSA Approved; OpaqueInformation Provided by Teknor Apex
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Teknor Apex Monprene® MP-2455N Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Teknor Apex Monprene® MP-2770L2 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Teknor Apex Sinpolene CPP1030 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Teknor Apex Sinpolene CPP2020 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 20% Filler by Weight Features: Copolymer Uses: Furniture Forms: PelletsInformation Provided ..
|
|||
| Melt Flow |
10.0
-
30.0
g/10 min <br>@Load 10.0 kg,<br> Temperature 190 °C
|
10.0
-
30.0
g/10 min <br>@Load 22.0 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
Teknor Apex Sinpolene MBB1512 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (350000 ppm) Features: General Purpose Uses: Non-specific Food Applications Forms: Pellets Pro..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
Teknor Apex Sinpolene MBW108LE Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Uses: Film; Sheet Forms: Pellets Processing Method: Injection Molding;..
|
|||
| Melt Flow |
10.0
-
30.0
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
10.0
-
30.0
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Teknor Apex Sinpolene MBW1475 Specialty Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor ..
|
|||
| Melt Flow |
10.0
-
30.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
-
30.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Teknor Apex Sinpolene MBW5335 Specialty Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (200000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Teknor Apex Synres® PP HFR005 Polypropylene
Notes: The Specialty Compounding Division offer a proprietary line of flame retardant polyolefins. Typical applications include building products, electrical/electronic and many other consumer and i..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Entec Hypro™ PPC-CC40 Natural Copolymer Polypropylene, 40% Calcium Carbonate Filled
Information provided by Entec
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Entec Hypro™ PPC-GF10 Natural Impact Polypropylene, 10% Glass Reinforced
Information provided by Entec
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Entec Hypro™ PPC-GF25 Natural Impact Polypropylene, 25% Glass Reinforced
Information provided by Entec
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Entec Hypro™ PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled
Information provided by Entec
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Entec Hypro™ PPC-GF40 Natural Impact Polypropylene, 40% Glass Reinforced
Information provided by Entec
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
10.0
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D1238 |
|
Bhansali Engineering Abstron TIM 300 MMA- ABS
High Impact(Transparent ABS)Information provided by Bhansali
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
10.0
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Teknor Apex Elexar® EL 8730R Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Teknor Apex Sinpolene CPP1020 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 20% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
Teknor Apex Sinpolene MBW0442 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Filler/Reinforcement: Calcium Carbonate Filler Uses: Film Forms: Pelle..
|
|||
| Melt Flow | 10.0 - 14.3 g/10 min | 10.0 - 14.3 g/10 min | Average value: 12.4 g/10 min Grade Count:3 |
|
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Melt Flow |
10.0
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
10.0
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
Teknor Apex Monprene® MP-2785H Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||