| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 230 °C |
13
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Multibase Multi-Pro® 5012 C Natural Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingFeatures:Gloss, LowInformation provided by Multibase
|
|||
| Melt Flow |
13
g/10 min @Load 5.00 kg, Temperature 260 °C |
13
g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Melt Flow |
13
g/10 min @Load 1.20 kg, Temperature 300 °C |
13
g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® AD143 PC (Europe-Africa-Middle East)
LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission ..
|
|||
| Melt Flow |
13
g/10 min @Load 1.20 kg, Temperature 300 °C |
13
g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Asia Pacific)
Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co..
|
|||
| Melt Flow | 13 g/10 min | 13 g/10 min | |
|
Custom Resins Duratel™ MF13 Acetal Copolymer
(discontinued **)
Description: Duratel™ MF13 is a 13 melt flow, general purpose acetal copolymer. Information provided by Custom Resins.
|
|||
| Melt Flow | 13 g/10 min | 13 g/10 min | 230/2.16 (typical); ASTM D1238 |
|
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Melt Flow |
13
g/10 min @Load 5.00 kg, Temperature 250 °C |
13
g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
|
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
|
|||
| Melt Flow |
13
g/10 min @Load 5.00 kg, Temperature 250 °C |
13
g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
|
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
|
|||
| Melt Flow |
13
g/10 min @Load 10.0 kg, Temperature 220 °C |
13
g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
|
Styrolution Absolac® 30GF15 ABS, 15% Glass Filled
15% glass filledInformation provided by Styrolution
|
|||
| Melt Flow |
13
g/10 min @Load 5.00 kg, Temperature 280 °C |
13
g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
|
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific)
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 230 °C |
13
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
SK Chemicals SKYPEL G172D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 230 °C |
13
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Borealis BE170MO Polypropylene Copolymer
BE170MO is a heterophasic copolymer. This grade is characterized by high impact strength, high stiffness and good flow properties. This grade contains additives providing low taste and odor as well..
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 230 °C |
13
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Borealis Bormed™ BE860MO Polypropylene Copolymer for Healthcare Applications
Bormed BE860MO is a heterophasic copolymer characterized by an excellent impact strength also at low temperatures (deep freeze applications) together with high stiffness and good flow properties.Bor..
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 230 °C |
13
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer
BorPure™ RE450MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is characterized by optimum combination of high impact strength and..
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 230 °C |
13
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Borealis Daplen™ EE188HP Polypropylene TPO Compound
Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g..
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 190 °C |
13
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
A. Schulman POLYBATCH™ Violet 4022 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 4022 is a violet color concentrate based in polyethylene. This masterbatch was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH®..
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 230 °C |
13
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled)
DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman.
|
|||
| Melt Flow |
13
g/10 min @Load 10.0 kg, Temperature 220 °C |
13
g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
|
Cossa Polimeri ESTALUX 5513 Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
|
|||
| Melt Flow |
13
g/10 min @Load 1.20 kg, Temperature 300 °C |
13
g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
|
Covestro Makrolon® 2665 MAS071 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med..
|
|||
| Melt Flow | 13 g/10 min | 13 g/10 min | ISO 1133 |
|
ExxonMobil Exxtral™ BMU 139 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci..
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 190 °C |
13
g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
|
DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal (POM)
(Unverified Data**)
X-ray Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400XRD NC010 is a filled medium viscosity acetal copolymer for injection molding. It is detected i..
|
|||
| Melt Flow |
13
g/10 min @Load 1.20 kg, Temperature 300 °C |
13
g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
|
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFlame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2..
|
|||
| Melt Flow |
13
g/10 min @Load 1.20 kg, Temperature 300 °C |
13
g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
|
E-Polymers TEKANATE® G7013FR General Purpose Easy Molding Flame Retardant Polycarbonate
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows ..
|
|||
| Melt Flow | 13 g/10 min | 13 g/10 min | ASTM D1238 |
|
Aclo Accutech Polypropylene Copolymer CP0437G20CL Glass Reinforced Coupled |
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 190 °C |
13
g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
|
BASF Ultraform® S2320 0035 POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF
|
|||
| Melt Flow |
13
g/10 min @Load 5.00 kg, Temperature 200 °C |
13
g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
|
Americas Styrenics MC3650 High Heat Crystal Polystyrene
Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer..
|
|||
| Melt Flow | 13 g/10 min | 13 g/10 min | ASTM D1238 |
|
Asahi Kasei Thermofil P-40TC-0158 40% Talc Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Melt Flow |
13
g/10 min @Load 2.16 kg, Temperature 190 °C |
13
g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
|
BASF Ultraform® S2320 003 PRO POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
|
|||
| Melt Flow | 13 g/10 min | 13 g/10 min | Condition I; ASTM D1238 |
|
Asahi Kasei Delpet® 560F Acrylic Molding Compound
560F has the highest flow of Delpet® grades, allowing reduced screw load for broad selection of molding conditions. General Delpet® qualities include attractive transparency, elegant luster and c..
|
|||