Physical Properties Metric English Comments
Melt Flow 2.3 g/10 min
<br>@Temperature 190 °C
2.3 g/10 min
<br>@Temperature 374 °F
North Wood Plastics HDPE with 40% Wood Fiber
Data provided by North Wood Plastics, Inc.
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
NOVA Chemicals Novapol® LF-0224-A LDPE &nbsp;(discontinued **)
Puncture value is 43.2 J/mm. LDPE. Excellent stiffness, moderate toughness, easy processability. Additive Package: Base Resin.Applications: Industrial packaging, liners, blends with LLDPE, foam art..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ISO 1133
Yparex 8102 Polyolefin Adhesive Resin
The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer..
Melt Flow 2.3 g/10 min
2.3 g/10 min
Exxon Method
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin &nbsp;(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
M. Holland Company LD219AA LDPE &nbsp;(discontinued **)
Features: Good Processability, Ultra High ToughnessUses: Bottles, PackagingProcessing Method: Blow MoldingInformation provided by M. Holland.
Melt Flow 2.3 g/10 min
2.3 g/10 min
Exxon Method
ExxonMobil Escorene® LD-768 High EVA Film and Compounding Resin &nbsp;(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low gel 27.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming
COPYLENE™ CH023NX has a high performance nucleation system designed to yield high clarity thermoformed articlesApplications: ThermoformingInformation provided by Phillips 66.
Melt Flow 2.3 g/10 min
2.3 g/10 min
ISO 1133
Lucite International Diakon® TD642 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Melt Flow 2.3 g/10 min
<br>@Load 6.60 kg,<br> Temperature 337 °C
2.3 g/10 min
<br>@Load 14.6 lb,<br> Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific)
20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.
Melt Flow 2.3 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
2.3 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade
Information provided by Samsung Cheil Industries.
Melt Flow 2.3 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
2.3 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Flow 2.3 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
2.3 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade
Information provided by Samsung Cheil Industries.
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Westlake EF706 Low Density Polyethylene
Westlake EF706 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ISO 1133
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film
LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of..
Melt Flow 2.3 g/10 min
<br>@Temperature 230 °C
2.3 g/10 min
<br>@Temperature 446 °F
I&lt;sub&gt;2&lt;/sub&gt;; ASTM D1238
Formosa Plastics Formolene® 3302B Random Copolymer Polypropylene
Random Copolymer for Extrusion and Thermoforming Applications Formolene® 3302B is a low melt flow random with excellent clarity, fast cycle time and easy mold release, designed for extrusion proces..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin
Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North ..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin
Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd..
Melt Flow 2.3 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
2.3 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
Entec Hylex® P1302B Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Melt Flow 2.3 g/10 min
2.3 g/10 min
ASTM D1238
Dow DOWLEX™ 2247G Polyethylene Resin
Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg
2.3 g/10 min
<br>@Load 4.76 lb
Melt flow ratio I10/I2 is 7.3.
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
ExxonMobil Escorene™ 768.MJ Blown Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 768.MJ is a low gel 26.2% vinyl acetate copolymer designed for film and compounding applications. This resin provides very low modulus films with high tensile ..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM-D1238
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer
FL31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processing ..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 235 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 455 °F
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Conditioned)
Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Stretch film; shrink film; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Braskem LH218 Linear Low Density Polyethylene
Insulation for low and medium tension XLPE wires and cables.Information provided by Braskem.
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene
Description: LL218 is a Linear Low Density Polyethylene, copolymer of butene-1, produced by Spherilene process. Developed for cast film extrusion. Films obtained with this product show a good proces..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Bapolene® 270F Low Density Polyethylene Film Extrusion Resin
Bapolene® 270F is an LDPE for blown film requiring superior clarity. It contains 1600 ppm antiblock and 725 ppm slip additives. This product meets the Food and Drug Administration requirements of ..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ISO 1133
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film
LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene..
Melt Flow 2.3 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.3 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® 300ATB BK000 Acetal Homopolymer &nbsp;(Unverified Data**)
Delrin® 300ATB BK000 is a filled, medium viscosity, toughened acetal homopolymer for injection molding. It is well suited for antistatic applications.Information provided by DuPont Performance Poly..
Copyright © lookpolymers.com All Rights Reserved