| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
22
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
22
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East)
Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by ..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C
|
22
g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
|
|||
| Melt Flow |
22
g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C
|
22
g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F
|
ASTM D 1238 |
|
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS
FXC810MA is the grade code for the Marble effect in PC/ABS. Marble is part of the VisualFX portfolio, and it is offered in a range of colors simluating the Marble effect. High heat/good flow charact..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 2.16 kg,<br> Temperature 210 °C
|
22
g/10 min <br>@Load 4.76 lb,<br> Temperature 410 °F
|
|
|
Noltex Soarnol® BG3522 Ethylene Vinyl Alcohol Copolymer
Special designed high MFI grade. New EVOH for extrusion coating. Ethylene content 35 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, ..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® LUX7189 PC (Europe-Africa-Middle East)
Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems.
|
|||
| Melt Flow | 22 g/10 min | 22 g/10 min | ASTM D1238 |
|
LyondellBasell Microthene® G MN71020 Low Density Polyethylene
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
|
|||
| Melt Flow | 22 g/10 min | 22 g/10 min | ASTM D1238 |
|
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding)
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
|
|||
| Melt Flow | 22 g/10 min | 22 g/10 min | ASTM D1238 |
|
LyondellBasell Microthene® G MN72700 Low Density Polyethylene
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
22
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
M. Holland Company PP500 Polypropylene Homopolymer
Features: Homopolymer, Narrow Molecular Wt. Dist.Uses: Disposable Drinkware, Medical Applications, PackagingApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by ..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
22
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D1238 |
|
LG Chemical HI121U ABS
Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic..
|
|||
| Melt Flow | 22 g/10 min | 22 g/10 min | ASTM D1238 |
|
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin
Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon.
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin
Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 2.16 kg,<br> Temperature 250 °C
|
22
g/10 min <br>@Load 4.76 lb,<br> Temperature 482 °F
|
|
|
LG Chemical LUPOY GN-5001TF Halogen Free PC/ABS Alloy, High Flow, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East)
PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
|
|||
| Melt Flow |
22
g/10 min <br>@Load 10.0 kg,<br> Temperature 230 °C
|
22
g/10 min <br>@Load 22.0 lb,<br> Temperature 446 °F
|
|
|
Stellarchem SV-B75E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
Samsung Cheil Industries Infino® SC-1220R PC, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
Samsung Cheil Industries Infino® SC-1220UR PC, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ISO 1133; ASTM D1238 |
|
Styron CALIBREâ„¢ 201-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM Data |
|
Styron CALIBREâ„¢ 2071 15 Polycarbonate, Sterilization Grade
CALIBRE® 2071 resins are designed for those applications which use steam or ethylene oxide for sterilization while providing enhanced mold release characteristics. This material has excellent ret..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
22
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D1238 |
|
Samsung Cheil Industries Starex® WR-9100 ASA, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ISO 1133 |
|
Styron CALIBREâ„¢ 301EP-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 5.00 kg,<br> Temperature 250 °C
|
22
g/10 min <br>@Load 11.0 lb,<br> Temperature 482 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics NORYL PX1007 PPE+PS
Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade.
|
|||
| Melt Flow |
22
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
22
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
Styron CALIBREâ„¢ 301 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Melt Flow |
22
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
22
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
A. Schulman POLYBATCH™ Yellow 2057E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 2057E is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2057E is h..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
22
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
A. Schulman POLYBATCH™ Yellow 2057E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 2057E is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2057E is h..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
22
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
A. Schulman POLYBATCH™ Blue 4025 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® Blue 4025 is a blue color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 4025 is ..
|
|||
| Melt Flow |
22
g/10 min <br>@Load 2.16 kg,<br> Temperature 275 °C
|
22
g/10 min <br>@Load 4.76 lb,<br> Temperature 527 °F
|
ISO 1133 |
|
BASF Ultradur B 4406 G6 Q717 30% Glass Filled PBT
Ultradur B 4406 G6 Q717 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement.
|
|||
| Melt Flow |
22
g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C
|
22
g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F
|
ASTM Data |
|
Styron Magnum™ 9100 MFD ABS