| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
25
g/10 min <br>@Load 0.325 kg,<br> Temperature 270 °C
|
25
g/10 min <br>@Load 0.716 lb,<br> Temperature 518 °F
|
|
|
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre
FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
25
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
|
|
PTS Trilac® TR558-CL ABS- Transparent ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Flow |
25
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
25
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D 1238 |
|
SABIC Innovative Plastics Lexan® FXD171R PC
Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Melt Flow |
25
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
25
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® HF1140R PC (Asia Pacific)
LEXAN HF1140R is a high flow grade. This material is especially designed for applications that require thin wall sections and high flow lengths. FDA food contact compliant in limited colors. Effe..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
25
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® LSHF PC (Asia Pacific)
Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization
|
|||
| Melt Flow |
25
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
25
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® LSHF PC (Europe-Africa-Middle East)
Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization
|
|||
| Melt Flow |
25
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
25
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
STN EN ISO 1133 |
|
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted
FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C
|
25
g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F
|
ASTM D1238 |
|
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Melt Flow | 25 g/10 min | 25 g/10 min | Exxon Method |
|
ExxonMobil Escorene® LD-781 High EVA Compounding Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymer for specialty compounding applications. The resin provides excellent stress cracking and flexibility, and allows outs..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
25
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ISO 1133 |
|
MBA Polymers PP 2172 Post-consumer recycled polypropylene copolymer
High melt flow rate for injection molding applications. Available in standard black.Information provided by MBA Polymers.
|
|||
| Melt Flow |
25
g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C
|
25
g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F
|
ASTM-D1238 |
|
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade
Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus..
|
|||
| Melt Flow | 25 g/10 min | 25 g/10 min | |
|
Intercontinental Polymers HoPBT 550 HoPBT Polymer Type - Clear, Polyester Pellets
Applications: Engineering Resin Information provided by Intercontinental Polymers.
|
|||
| Melt Flow |
25
g/10 min <br>@Load 2.16 kg,<br> Temperature 260 °C
|
25
g/10 min <br>@Load 4.76 lb,<br> Temperature 500 °F
|
Estimated using room temperature density; ISO 1133 |
|
Lanxess Pocan® B 3235 901510 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding
|
|||
| Melt Flow |
25
g/10 min <br>@Load 2.16 kg,<br> Temperature 400 °C
|
25
g/10 min <br>@Load 4.76 lb,<br> Temperature 752 °F
|
ASTM D1238 |
|
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 5.00 kg,<br> Temperature 266 °C
|
25
g/10 min <br>@Load 11.0 lb,<br> Temperature 511 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East)
VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage.
|
|||
| Melt Flow |
25
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
25
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Teknor Apex MONPRENE® MP 2790 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Melt Flow |
25
g/10 min <br>@Load 5.00 kg,<br> Temperature 250 °C
|
25
g/10 min <br>@Load 11.0 lb,<br> Temperature 482 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Europe-Africa-Middle East)
high gloss Noryl
|
|||
| Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238 |
|
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Melt Flow |
25
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
25
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
A. Schulman POLYBATCH™ Red 502 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 5020 is a bright red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5020 is..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
25
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D 1238 |
|
Cossa Polimeri ESTADIENE 3520 Acrylonitrile Butadiene Styrene
ABS with high impact resistanceHigh melt flow rate, high impact resistance at low temperature, excellent processability and surface appearanceInformation provided by Cossa Polimeri S.r.l.
|
|||
| Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238 |
|
ExxonMobil Escorene™ UL 02528CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 02528CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: YesFree ..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 5.00 kg,<br> Temperature 275 °C
|
25
g/10 min <br>@Load 11.0 lb,<br> Temperature 527 °F
|
ISO 1133 |
|
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
25
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Carmel Olefins CAPILENE® TT 75 AV Polypropylene Impact Copolymer
Description: CAPILENE® TT 75 AV is a nucleated, controlled rheology heterophasic copolymer designed for injection molding. It is characterized by excellent impact strength, even at low temperatur..
|
|||
| Melt Flow | 25 g/10 min | 25 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
|
EMS-Grivory Grivory® G 21 PA6I/6T
Product description: Grivory G 21 natural 6506 is a high viscosity, partially aromatic, amorphous copolyamide with processing aid. Improved gas and aroma barrier at elevated relative humidityExcelle..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
25
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ISO 1133 |
|
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**)
Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform..
|
|||
| Melt Flow | 25 - 30 g/10 min | 25 - 30 g/10 min | ASTM D1238 |
|
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Melt Flow |
25
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
25
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Lexan® HF1110 PC (Asia Pacific)
General purpose grade. Good clarity, heat resistance, property retention and dimensional stability.
|
|||
| Melt Flow | 25 - 50 g/10 min | 25 - 50 g/10 min | ASTM D1238 |
|
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Melt Flow |
25
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
25
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr..
|
|||
| Melt Flow |
25
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
25
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
|
|
Kraton® D1119 P (SIS) Linear Triblock Copolymer