Physical Properties Metric English Comments
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen EP300R Injection Molding Grade Polypropylene
Moplen EP300R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300R is a block copolymer particularly suitable for injection..
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Gichem GILAC H120X6/VOU ABS Flame Retardant &nbsp;(discontinued **)
ABS self-extinguishing class V0 with better fluidity and UV resistance. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Melt Flow 30 g/10 min
30 g/10 min
10% POSS® in PP
Hybrid Plastics MS0825 Nanoreinforced® POSS® Polypropylene
Nanoreinforced® polypropylene utilizes POSS® technology to achieve, increased hydrophobicity, lower coefficient of friction and improved processability through structural control at the nanome..
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Hyosung Topilene R801H PP
R801H Injection Random CopolymerApplications:High transparent productLarge articlesCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
LG Chemical KEYFLEX BT 5035D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
LG Chemical LUPOL HF5254A PP+MF20%
Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
L; ASTM D1238
Global PP-2340-S Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-electrical appliances, bases, panels, auto parts, cupsInformation provided by Global Polymers Corpo..
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Inno-Comp INNOPOL® CS 2-9301 Elastomer Modified Polypropylene Block-Copolymer
INNOPOL® CS 2-9301 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9301 is developed for produ..
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
IRPC Polimaxx Polene 2300SC Polypropylene Block Copolymer
CHARACTERISTICS: HIGH FLOW, GOOD IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, THIN WALL PARTS
Melt Flow 30 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
30 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Flow 30 g/10 min
<br>@Load 5.00 kg,<br> Temperature 260 °C
30 g/10 min
<br>@Load 11.0 lb,<br> Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East)
Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only.
Melt Flow 30 g/10 min
<br>@Load 10.0 kg,<br> Temperature 250 °C
30 g/10 min
<br>@Load 22.0 lb,<br> Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact
High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries.
Melt Flow 30 g/10 min
<br>@Load 10.0 kg,<br> Temperature 250 °C
30 g/10 min
<br>@Load 22.0 lb,<br> Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow >= 30 g/10 min
<br>@Load 10.0 kg,<br> Temperature 220 °C
>= 30 g/10 min
<br>@Load 22.0 lb,<br> Temperature 428 °F
ISO 1133
Styrolution Absolan® 2300 SAN
Absolac 2300 is a good flow gradeInformation provided by Styrolution
Melt Flow 30 g/10 min
<br>@Temperature 230 °C
30 g/10 min
<br>@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene
DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman.
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
UBE UMERIT 613A Metallocene LLDPE
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert..
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Borealis RG435MO Polypropylene, Transparent Random Copolymer
RG435MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. Products molded from this grade exhibit excellent transparency, good gloss, high impact..
Melt Flow 30 - 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 - 35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer
DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman.
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
ExxonMobil PP8255E1 Polypropylene Homopolymer
Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes...
Melt Flow 30 g/10 min
<br>@Load 5.00 kg,<br> Temperature 265 °C
30 g/10 min
<br>@Load 11.0 lb,<br> Temperature 509 °F
ASTM D1238
Diamond Polymers ASAPC 6141 UV Stabilized
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Braskem 52T30V Homopolymer Polypropylene
Description: Clarified, Excellent Mold Release, Excellent Flow CharacteristicsApplications: Suggested Uses Include Housewares, Storage Boxes, Containers, VialsInformation provided by Braskem
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Braskem PB 608 LDPE Injection Molding Polyethylene
Description: PB608 is a grade produced under high pressure in an autoclave reactor. This grade is especially designed for injection molding of articles that must show excellent flexibility propertie..
Melt Flow 30 g/10 min
<br>@Load 5.00 kg,<br> Temperature 275 °C
30 g/10 min
<br>@Load 11.0 lb,<br> Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Melt Flow 30 g/10 min
<br>@Load 5.00 kg,<br> Temperature 275 °C
30 g/10 min
<br>@Load 11.0 lb,<br> Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
Melt Flow 30 g/10 min
<br>@Load 10.0 kg,<br> Temperature 220 °C
30 g/10 min
<br>@Load 22.0 lb,<br> Temperature 428 °F
ASTM D-1238
Bhansali Engineering Abstron HCR-15 M ABS Heat Resistant
Chemical Resistant GradeInformation provided by Bhansali
Melt Flow 30 - 45 g/10 min
<br>@Load 2.16 kg,<br> Temperature 250 °C
30 - 45 g/10 min
<br>@Load 4.76 lb,<br> Temperature 482 °F
ISO 1133
BLUESTAR PBT 1100
PBT resin is polymerized by pure terephthalic acid (PTA) and 1,4-butanediol (1,4-BDO) through direct esterification. With well-distributed molecular weight and stable quality, PBT resin possesses go..
Melt Flow 30 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
30 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM-D1238
Braskem G803 LDPE Injection Molding Polyethylene
G803 is a low-density polyethylene with excellent processability, high fluidity, and dimensional stability. It does not contain additives. Its applications include: lids, closures, and general purp..
Melt Flow 30 g/10 min
30 g/10 min
Zylog Hipolyene® 8110 EX Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Melt Flow 30 - 50 g/10 min
<br>@Load 21.6 kg,<br> Temperature 170 °C
30 - 50 g/10 min
<br>@Load 47.6 lb,<br> Temperature 338 °F
DDIN 53.735
Lubrizol Advanced Materials Pearlbond® 118 Thermoplastic Polyurethane
The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo..
Melt Flow 30 g/10 min
<br>@Load 2.16 kg
30 g/10 min
<br>@Load 4.76 lb
ASTM D1238
Reliance Industries Reclair M24300 Polyethylene
High flow Linear Low Density Polyethylene grade. Reclair M24300 is butene comonomer based, with optimum levels of antioxidants.Characteristics:narrow molecular weight distribution, good fluidity, ..