Polymer Property : Melt Flow = 34 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers NPP 20-3401 C/AS
Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers NPP 20-3401 NC
Description: Random Copolymer Polypropylene, Non ClarifiedInformation provided by Network Polymers Inc.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 260 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 260 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 260 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® RCY6013 PC+ABS (Asia Pacific)
Cycoloy* RCY6013 resin is an injection moldable high flow PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 @ 1.5 mm..
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Radici Heraflex® E 4718 TPC-ET Thermoplastic Elastomer
TPC-ET Thermoplastic Elastomer. Low Modulus, Nominal Shore D/15s 43. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene
Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f..
Melt Flow 34 g/10 min
34 g/10 min
ISO 1133
Solvay Engineered Polymers SEQUEL® 1490 Engineered Polyolefin &nbsp;(discontinued **)
Description: SEQUEL® 1490 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p..
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer
TPC-ET Thermoplastic Elastomer. Lowest Modulus, Nominal Shore D/15s 35. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Melt Flow 34 g/10 min
<br>@Load 3.80 kg,<br> Temperature 260 °C
34 g/10 min
<br>@Load 8.38 lb,<br> Temperature 500 °F
ASTM D1238
Ravago Manufacturing Americas Hybrid B2035I Polycarbonate + PBT Alloy
Available in North America High Impact Resistance Form: PelletsInformation provided by Ravago
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
LG Chemical SEETEC H7700 Polypropylene, Homopolymer
Features: Seetec H7700 is designed for the extrusion of fine fibers with the spunbond technology. This grade is characterized by very narrow molecular weight distribution (MWD), with anti-gas fading..
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 260 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 500 °F
Estimated using room temperature density; ISO 1133
Lanxess Pocan® B 3215 Z 000000 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding, impact modified
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 260 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 500 °F
ISO 1133-1
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres
PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS.
Melt Flow 34 g/10 min
<br>@Load 5.00 kg,<br> Temperature 270 °C
34 g/10 min
<br>@Load 11.0 lb,<br> Temperature 518 °F
Estimated using room temperature density; ISO 1133
Lanxess Pocan® T 3150 XF 000000 PBT + PET, 55% Glass Fiber
PBT+PET, 55% glass fibers, injection molding, improved flowability, low tendency to warp, increased temperature peak load, increased strength and increased modulus
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Condition L; ASTM D1238
LyondellBasell Pro-faxâ„¢ PH835 Polypropylene Homopolymer
Description: Pro-faxâ„¢ PH835 is a very high melt flow, controlled rheology polypropylene homopolymer resin designed for spunbond and continuous filament applications that require superior spinna..
Melt Flow 34 g/10 min
34 g/10 min
ASTM D1238
LyondellBasell Alathon® H5234 High Density Polyethylene
ApplicationsALATHON H 5234 is a high flow injection molding grade of resin designed for fast cycle and thin wall molding. It provides cold temperature impact resistance. Typical applications inclu..
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Ineos L34N-00 Polypropylene Impact Copolymer
Grade L34N-00 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in..
Melt Flow 34 - 40 g/10 min
<br>@Load 5.00 kg,<br> Temperature 365 °C
34 - 40 g/10 min
<br>@Load 11.0 lb,<br> Temperature 689 °F
ASTM D1238
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
Melt Flow 34 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
34 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
Samyang Trirex® 3017PJ Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP
LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include:..
Melt Flow 34 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
34 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
Samyang Trirex® 3017IR Polycarbonate with Heat Stabilizer
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017IR is a super high flow grade with added heat stabilizers, separating materials and..
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Melt Flow 34 g/10 min
<br>@Load 10.0 kg,<br> Temperature 220 °C
34 g/10 min
<br>@Load 22.0 lb,<br> Temperature 428 °F
ISO 1133
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene
Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
A. Schulman PP 1930-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930-01 is an automotive recognized copolymer polypropylene for use on interior trim applications.Information provided by A. Schulman.
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Braskem CP360H Homopolymer Polypropylene
Description: Narrow MWD, Low Smoke / CondensateApplications: Suggested Uses Include Fine Denier Spunbond Nonwovens, High-Speed Spinning - Continuous Filament YarnThis resin meets the requirements fo..
Melt Flow 34 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
34 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
LG Chemical SEETEC R7700 Polypropylene, Random Copolymer
Features: Seetec R7700 is designed for the extrusion of fibers with the spunbond technology. This grade is characterized by narrow MWD and good processability. SEETEC R7700 meets the FDA requirement..
Melt Flow 34 g/10 min
34 g/10 min
Melt Flow Ratio (I10/I2) is 7.3; ASTM D1238
Huntsman Rexell® H2104 Injection Molding LLDPE &nbsp;(discontinued **)
Linear-low high density homopolymer, injection molding, FDA compliant.Features: High flow and short cycle times.Applications: Thin wall containers.FDA Notes: Conforms to FDA regulation 21 CFR 177.15..