Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 35 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mytex Polymers AS33LW Polypropylene, Rubber modified, Talc filled, Compounded
Description: AS33LW is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and good ..
Melt Flow 35 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
35 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
Melt Flow 35 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
35 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Melt Flow 35 - 50 g/10 min
<br>@Load 11.6 kg,<br> Temperature 250 °C
35 - 50 g/10 min
<br>@Load 25.6 lb,<br> Temperature 482 °F
ASTM D1238
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Melt Flow 35 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
35 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Phillips 66 COPYLENE® CH350V Polypropylene, Homopolymer, Extrusion Coating, Spunbound, Gas Fade & UV Resistant
COPYLENE™ CH350V is a very high melt flow polypropylene homopolymer resin designed for fiber spinning. Applications: Food Packaging Film, Heavy Duty Packaging, Absorption & Filtration, Filament Yar..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Phillips 66 COPYLENE® CR350CL-02 Polypropylene, Random Copolymer, Clarified
CR350CL-02 is a clarified, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release.Potential Applications: Injection moldi..
Melt Flow 35 g/10 min
35 g/10 min
Condition L 230/2.16; ASTM D1238
Pinnacle Polymers 2135 H Medium Impact Polypropylene Copolymer, Injection Molding Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
M. Holland Company LL700 LLDPE &nbsp;(discontinued **)
Features: High ESCR (Stress Crack Resist.), Good Flexibility, High FlowUses: Closures, Household GoodsProcessing Method: Injection MoldingInformation provided by M. Holland.
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Gichem GILAC G160 Acrylonitrile Butadiene Styrene &nbsp;(discontinued **)
ABS very high fluidity, good resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Flint Hills P4C6Z-022 Homopolymer Polypropylene
Homopolymer, UL certified, and FDA compliant.Features: Controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Res..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Ineos H35Z-GP Polypropylene Homopolymer
This is a general purpose homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsC..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Ineos R35C-02 Polypropylene Random Copolymer
Grade R35C-02 is a high clarity, lubricated random copolymer with a high flow rate. This material is designed for high-speed injection molding of medium- to thin-walled parts requiring excellent cla..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Inno-Comp INNOPOL® CS 2-9110 10% Talc-Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-9110 is a 10% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9110 is developed for producing..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer
INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is develop..
Melt Flow 35 g/10 min
<br>@Load 10.0 kg,<br> Temperature 250 °C
35 g/10 min
<br>@Load 22.0 lb,<br> Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced
Information provided by Samsung Cheil Industries.
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
A. Schulman POLYFORT™ PX 1040
Information provided by A. Schulman.
Melt Flow 35 g/10 min
<br>@Temperature 230 °C
35 g/10 min
<br>@Temperature 446 °F
I&lt;sub&gt;2&lt;/sub&gt;; ASTM D1238
Formosa Plastics Formolene® 6335N Impact Copolymer Polypropylene
Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6335N is an engineered, medium impact copolymer polypropylene. It was specifically developed to..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Yellow P20199/2 Concentrate Based In Copolymer PP
DescriptionPOLYBATCH® P20199/2 is a yellow color concentrate based in copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P20199/2 is typically ..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Yellow P20199/2 Concentrate Based In Copolymer PP
DescriptionPOLYBATCH® P20199/2 is a yellow color concentrate based in copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P20199/2 is typically ..
Melt Flow 35 g/10 min
<br>@Temperature 230 °C
35 g/10 min
<br>@Temperature 446 °F
I&lt;sub&gt;2&lt;/sub&gt;; ASTM D1238
Formosa Plastics Formolene® 3335E Random Copolymer Polypropylene
Random Copolymer for Clear Storage Boxes, Pill Vials and Containers Formolene® 3335E is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for injection mo..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238, ISO 1133
DuPont™ Elvaloy® 741WR Ethylene/Vinyl Acetate/Carbon Monoxide (E/VA/CO) Copolymer
DuPont™ Elvaloy® 741WR an ethylene/vinyl acetate/carbon monoxide (E/VA/CO) copolymer. The difference between Elvaloy®741 and Elvaloy®741WR, is that Elvaloy®741WR contains a wax additive to dete..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
ExxonMobil PP7035E4 Impact Copolymer
Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional ..
Melt Flow 35 g/10 min
<br>@Temperature 230 °C
35 g/10 min
<br>@Temperature 446 °F
ASTM D1238
Dow C700-35 Polypropylene Resin
DOW C700-35 is intended for use in injection molding processes where medium impact strength is required.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in J..
Melt Flow 35 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
35 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
Clariant Renol CPS04230 Color concentrate of Titanium Oxide
Application to PolystyreneData provided by Clariant Masterbatches
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Bapolene® PP5083 Polypropylene, Injection Grade
Bapolene PP 5083 is a clarified PP Random Copolymer for injection molding. This resin exhibits good processing and impact properties. This product meets FDA regulation 21CFR 177.1520 and is suitab..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ISO 1133
BASF Ultraform® W2320 U035 LEV POM
Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
LyondellBasell Pro-fax SG802N Polypropylene Impact Copolymer
Key Features: high flow, high impact polypropylene copolymer resin, excellent cold impact resistance, good stiffness and impact balance, UV stabilizer compatibilityApplications: automotive interior ..
Melt Flow 35 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
35 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Ineos H35G-00 Polypropylene Homopolymer
This is a general purpose homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsC..
Copyright © lookpolymers.com All Rights Reserved