Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 35 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 1.20 kg,
Temperature 300 °C
35 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin
Molded Plaque Properties. Features: High flow, Granular, Improved dispersion concentrates.Applications: housewares, additive and color, masterbatches/compounding.Data provided by the manufacturer.
Melt Flow 35 g/10 min

@Load 1.20 kg,
Temperature 300 °C
35 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LL 6235.19 Injection Molding Resin  (discontinued **)
LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in ..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Phillips 66 COPYLENE® CM350LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding
COPYLENE™ CM350LN is a high melt flow, controlled rheology, medium impact polypropylene copolymer resin designed for injection molding applications requiring a good balance of stiffness, impact, re..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
BP Amoco Acctuf® 3950 Impact Copolymer Polypropylene  (discontinued **)
Suggested fabrication methods: Injection moldingFeatures: Low gloss, High melt flow, Low temp impact, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fro..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
M. Holland Company PP710 Polypropylene Homopolymer
AntistaticHomopolymerNarrow molecular wt. dist.NucleatedApplications: CapsClosuresConsumer applications
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Flint Hills P4C6Z-059 Homopolymer Polypropylene
Homopolymer, UL certified, and FDA compliant.Features: Controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Res..
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Flint Hills P5M6K-048 Random Copolymer Polypropylene
Random copolymer, FDA compliant.Features: Clarified (50 mil plaque haze 10%), antistat, and controlled rheology.Applications: Injection molding: high clarity parts, medical parts, and good organole..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
MBA Polymers PP 2182 Post-consumer recycled polypropylene copolymer
Very high melt flow rate for injection molding application. Available in standard black.Information provided by MBA Polymers.
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ineos R35C-01 Polypropylene Random Copolymer
Grade R35C-01 is a high clarity random copolymer with a high flow rate. This material is designed for high speed injection molding and meets the requirements of the U.S. Food and Drug Administration..
Melt Flow 35 g/10 min

@Load 5.00 kg,
Temperature 260 °C
35 g/10 min

@Load 11.0 lb,
Temperature 500 °F
Calculated from MVR using melt density; ISO 1133
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
JPJ Technologies PP H35S Homopolymer for Injection Molding
PP H35S is specifically developed for producing injection molding articles for general purpose applications. It gives consistent processability and high gloss in the products. Application: General u..
Melt Flow 35 g/10 min

@Load 5.00 kg,
Temperature 230 °C
35 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Multibase Multibatch® MP 52214 Injection Molding
HPP. 75% CaCO3, 10%TiO2FilledFine Particle Size.Information provided by Multibase
Melt Flow 35 g/10 min

@Load 10.0 kg,
Temperature 220 °C
35 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® NH-1907 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Styron LGF 7600 Polypropylene
Overview: STYRON LGF7600 is intended for use injection molding applications that require high stiffness. The material has good processability and fast cycle times. It contains nucleating agent. LGF ..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene
DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided ..
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
UBE J3519 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Green P30244/4 Concentrate Based In Copolymer PP
DescriptionPOLYBATCH® P30244/4 is a green color concentrate based in Copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P30244/4 is typically ..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Yellow P20199/2 Concentrate Based In Copolymer PP
DescriptionPOLYBATCH® P20199/2 is a yellow color concentrate based in copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P20199/2 is typically ..
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
A. Schulman PP 3479-01 Polypropylene Random Copolymer
DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding ..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl..
Melt Flow 35 g/10 min

@Temperature 230 °C
35 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Formosa Plastics Formolene® 6535N Impact Copolymer Polypropylene
Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6535N is an engineered, medium impact copolymer polypropylene. It was specifically developed to..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Green P30244/4 Concentrate Based In Copolymer PP
DescriptionPOLYBATCH® P30244/4 is a green color concentrate based in Copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P30244/4 is typically ..
Melt Flow 35 g/10 min

@Load 5.00 kg,
Temperature 224 °C
35 g/10 min

@Load 11.0 lb,
Temperature 435 °F
ASTM D1238
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low temperature impactAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Braskem FPT350WV3 Homopolymer Polypropylene
Description: Narrow molecular weight distribution, antistatic, nucleated, very good mold release.Applications: Suggested uses include fast-cycle injection molding, large-part injection molding, disp..
Melt Flow 35 g/10 min

@Load 10.0 kg,
Temperature 190 °C
35 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
BASF Ultraform® FK 61002 20% Carbon Black Filled POM
Description: Polyoxymethylene based batch with approx. 20% carbon black for coloring thermoplastic polyoxymethylenes. Recommended concentrations of FK61002 batch within the mixture with thermoplasti..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
LyondellBasell Pro-fax SG802N Polypropylene Impact Copolymer
Key Features: high flow, high impact polypropylene copolymer resin, excellent cold impact resistance, good stiffness and impact balance, UV stabilizer compatibilityApplications: automotive interior ..
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
BP Amoco Acclear® 8939 Random Copolymer Polypropylene, High Clarity Grade  (discontinued **)
Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Excellent static control, ToughenedTypical applications: Housewares, Rigid packaging, Media packag..