| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 230 °C |
36 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| NCMT NanoPAC™ HS403 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 190 °C |
36 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
| PolyOne Geon™ Vinyl Flexible XV3807 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 400 °C |
36 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
| Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 400 °C |
36 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
| Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 400 °C |
36 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
| Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 230 °C |
36 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Ineos H36G-00 Polypropylene Homopolymer This is a high flow rate homopolymer. This material is designed for fiber spinning and spun bonded processes. It meets the requirements of the U.S. Food and Drug Administration as specified in 21 .. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 230 °C |
36 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Ineos H36G-01 Polypropylene Homopolymer This is a polypropylene homopolymer for general purpose injection molding and high speed fiber spinning applications. It is useful for spunbonded nonwovens and partially oriented yarn (POY). This .. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 230 °C |
36 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 230 °C |
36 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
| Kuraray SEPTON® PM4 Polypropylene Modified Plastic Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
| Melt Flow | 36 g/10 min @Load 5.00 kg, Temperature 270 °C |
36 g/10 min @Load 11.0 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
| Lanxess Durethan® BKV 50 H2.0 EF 000000 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow) |
|||
| Melt Flow | 36 g/10 min @Load 5.00 kg, Temperature 270 °C |
36 g/10 min @Load 11.0 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
| Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates |
|||
| Melt Flow | 36 g/10 min @Load 5.00 kg, Temperature 260 °C |
36 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
| Lanxess Pocan® C 3230 XF 000000 PBT + PC, 30% Glass Fiber PBT+PC, 30% glass fibers, injection molding, improved flowability, low tendency to warp, improved surface finish |
|||
| Melt Flow | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
nominal; ASTM D1238 |
| MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 400 °C |
36 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
| Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK) KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 400 °C |
36 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
| Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 400 °C |
36 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
| Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 400 °C |
36 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
| Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK) KetaSpire® KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standard.. |
|||
| Melt Flow | 36 g/10 min @Load 10.0 kg, Temperature 250 °C |
36 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
| Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Melt Flow | 36 g/10 min @Load 10.0 kg, Temperature 250 °C |
36 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
| Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Melt Flow | 36 g/10 min | 36 g/10 min | Cond. E; ASTM D1238 |
| DuPont Conpol™ 4R11S1 Ethylene-Methacrylic Acid Additive Resin Conpol™ additive resins, supplied in pellet form, are designed to modify the surface properties of films or coatings of Surlyn® ionomer resins and Nucrel® acid copolymer resins. They are concentr.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 230 °C |
36 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| ExxonMobil PP3155 Homopolymer Grade for Nonwoven and Fiber Applications Product Description: A homopolymer resin designed for spunbond nonwovens. The resin is particularly suited for excellent spinning for uniform, high quality fabrics.Availability: North America and S.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 230 °C |
36 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| ExxonMobil PP3155E3 Polypropylene Copolymer Product Description: A homopolymer resin designed for spunbond nonwovens. The resin is particularly suited for excellent spinning for uniform, high quality fabrics.Availability: Asia Pacific Featur.. |
|||
| Melt Flow | 36 g/10 min @Load 2.16 kg, Temperature 230 °C |
36 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Phillips 66 COPYLENE® CM360N Polypropylene, Impact Copolymer, Injection Molding COPYLENE® CM360N is a high melt flow, no-break impact polypropylene copolymer resin designed for injection molding applications requiring a good balance of stiffness, impact, resistance and process.. |
|||