| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
Procedure A Condition E; ASTM D1238 |
|
Network Polymers NPP 11-5026
Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc.
|
|||
| Melt Flow | 50 g/10 min | 50 g/10 min | I<sub>21</sub>; ASTM D238 |
|
Petromont 2200 High Density Polyethylene Resin
Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring impr..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 250 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 482 °F
|
ISO 1133 |
|
DuPont Performance Polymers Crastin® CE2055 NC010 PBT
(Unverified Data**)
Crastin® CE2055 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
ExxonMobil LL 6201 Injection Molding Resin
(discontinued **)
LL 6201 is a narrow molecular weight butene copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications ..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin
(discontinued **)
Features: Excellent processability for applications requiring moderate stiffness and improved toughnessExcellent cold temperature impact properties Applications: Ice cream containersHousewares Deep..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 5.00 kg,<br> Temperature 380 °C
|
50
g/10 min <br>@Load 11.0 lb,<br> Temperature 716 °F
|
|
|
Lehmann & Voss LUVOCOM® 1105-7197/BK PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade
ALATHON H4250 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p..
|
|||
| Melt Flow | 50 - 80 g/10 min | 50 - 80 g/10 min | Melt Volume Rate (cm³/10 min) |
|
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether
Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS..
|
|||
| Melt Flow |
>=
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
>=
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
|
|
Lehmann & Voss LUVOCOM® 94-8485 LD-PE, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable ..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
IRPC Polimaxx Polene 2541TC Polypropylene Block Copolymer
CHARACTERISTICS: EXCELLENT FLOWABILITY, HIGH STIFFNESS, HEAT STABILITY, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING SPECIALLY FOR WASHING TUB, ELECTRICAL APPLIANCES, THIN WALL CONTAINERS
|
|||
| Melt Flow |
50
g/10 min <br>@Load 5.00 kg,<br> Temperature 250 °C
|
50
g/10 min <br>@Load 11.0 lb,<br> Temperature 482 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 10.0 kg,<br> Temperature 250 °C
|
50
g/10 min <br>@Load 22.0 lb,<br> Temperature 482 °F
|
ASTM D1238 |
|
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
|
|
Silon Tabond 5007 Adhesive Resin
Tabond 5007 is a chemically modified Polypropylene. Its functional groups improve considerably the bonding between polar polymers, metals and glass.Characteristics: • Strong adhesion to aminosi..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 5.00 kg,<br> Temperature 280 °C
|
50
g/10 min <br>@Load 11.0 lb,<br> Temperature 536 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics NORYL PVX0901 PPE+PS (Asia Pacific)
Multi purpose V1 grade
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ISO 1133 |
|
Borealis Bormed™ BH348MO Polypropylene Heteroplastic Copolymer for Injection Molding
Bormed™ BH348MO is a polypropylene copolymer characterized by high impact strength, fast flow and crystallization speed. The material is nucleated with Borstar® Nucleation Technology (BNT). This ..
|
|||
| Melt Flow |
50
g/10 min <br>@Temperature 230 °C
|
50
g/10 min <br>@Temperature 446 °F
|
ASTM D1238 |
|
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
|
|||
| Melt Flow |
50
g/10 min <br>@Temperature 230 °C
|
50
g/10 min <br>@Temperature 446 °F
|
ASTM D1238 |
|
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
|
|||
| Melt Flow |
50
g/10 min <br>@Temperature 230 °C
|
50
g/10 min <br>@Temperature 446 °F
|
I<sub>2</sub>; ASTM D1238 |
|
Formosa Plastics Formolene® 6550A Thin Walled Injection Molding Polypropylene
Impact CopolymerApplications: Housewares, containers and other rigid packaging.Formolene 6550A (DEVELOPMENTAL) is a medium impact, high flow, controlled rheology copolymer of polypropylene designed ..
|
|||
| Melt Flow |
>=
50
g/10 min <br>@Load 10.0 kg,<br> Temperature 240 °C
|
>=
50
g/10 min <br>@Load 22.0 lb,<br> Temperature 464 °F
|
ISO 1133 |
|
Cossa Polimeri ESTABLEND PA 6000 ABS / Nylon 6 Blend
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
50
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D 1238 |
|
Cossa Polimeri ESTADIENE 1050 AS Acrylonitrile Butadiene Styrene
General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
ExxonMobil LLDPE LL 6201RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6201 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg
|
50
g/10 min <br>@Load 4.76 lb
|
Melt flow ratio I10/I2 is 8.5. |
|
Dow DOWLEX™ IP-50 High Density Polyethylene
DOWLEX® IP-50 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution designed for thin wall food containers. This resin is recommended for flo..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 5.00 kg,<br> Temperature 275 °C
|
50
g/10 min <br>@Load 11.0 lb,<br> Temperature 527 °F
|
ISO 1133 |
|
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural
Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn..
|
|||
| Melt Flow | 50 g/10 min | 50 g/10 min | ASTM D-1228 |
|
Bapolene® 2292 Polyethylene Film Grade
Bapolene 2292 is a butene linear low density polyethylene copolymer designed to provide a combination of toughness and stiffness and complies with FDA 21 CFR177.1520.Applications: Closures, lids, an..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ISO 1133 |
|
Carmel Olefins IPETHENE® 900 Low Density Polyethylene
IPETHENE® 900 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits high melt flow rate, good transparency, and flexibility. ..
|
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 275 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 527 °F
|
ISO 1133 |
|
BASF Ultradur B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET |
|||
| Melt Flow |
50
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
50
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ASTM D-1238 |
|
Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
| Melt Flow |
50
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
50
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
Braskem TI6500WV High Impact Copolymer Polypropylene
Description: High melt flow, superior low temperature impact, nucleated, good mold release, antistatic.Applications: Suggested uses include compounding, furniture, toys, packaging, large part inject..
|
|||