Physical Properties Metric English Comments
Melt Flow 30 - 50 g/10 min
30 - 50 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE A 7727 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Melt Flow 46 - 50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
46 - 50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers NPP 50-5052
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Melt Flow 38 - 50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
38 - 50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PP 8348S (EPH31RA) Propylene and Ethylene Block Polymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r..
Melt Flow 25 - 50 g/10 min
<br>@Load 5.00 kg,<br> Temperature 250 °C
25 - 50 g/10 min
<br>@Load 11.0 lb,<br> Temperature 482 °F
ASTM D1238
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy
PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Melt Flow 25 - 50 g/10 min
<br>@Load 5.00 kg,<br> Temperature 250 °C
25 - 50 g/10 min
<br>@Load 11.0 lb,<br> Temperature 482 °F
ASTM D1238
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant
PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
Melt Flow 25 - 50 g/10 min
<br>@Load 11.6 kg,<br> Temperature 250 °C
25 - 50 g/10 min
<br>@Load 25.6 lb,<br> Temperature 482 °F
ASTM D1238
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Melt Flow 35 - 50 g/10 min
<br>@Load 11.6 kg,<br> Temperature 250 °C
35 - 50 g/10 min
<br>@Load 25.6 lb,<br> Temperature 482 °F
ASTM D1238
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Melt Flow 25 - 50 g/10 min
<br>@Load 11.6 kg,<br> Temperature 250 °C
25 - 50 g/10 min
<br>@Load 25.6 lb,<br> Temperature 482 °F
ASTM D1238
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow
Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani..
Melt Flow 25 - 50 g/10 min
<br>@Load 5.00 kg,<br> Temperature 250 °C
25 - 50 g/10 min
<br>@Load 11.0 lb,<br> Temperature 482 °F
ASTM D1238
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Melt Flow 38 - 50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
38 - 50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PP 8340S (EPYH31U) Propylene and Ethylene Block Polymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r..
Melt Flow 38 - 50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
38 - 50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem PCC 4414 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Melt Flow 25 - 50 g/10 min
<br>@Load 5.00 kg,<br> Temperature 190 °C
25 - 50 g/10 min
<br>@Load 11.0 lb,<br> Temperature 374 °F
ISO 1133
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane
Pearlbondâ„¢ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ..
Melt Flow 30 - 50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 150 °C
30 - 50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 302 °F
Taiwan Sheen Soon Sheenthane® AH-661 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Melt Flow 25 - 50 g/10 min
25 - 50 g/10 min
Daikin NEOFLON RP-4020 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Melt Flow 25 - 50 g/10 min
<br>@Load 5.00 kg,<br> Temperature 275 °C
25 - 50 g/10 min
<br>@Load 11.0 lb,<br> Temperature 527 °F
ISO 1133
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar.
Melt Flow 0.30 - 50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
0.30 - 50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Aaron Industries AAROLENE® ARPE HD 300-2 High Density Polyethylene Compounded Resin
AAROLENE® ARPE 300 Series Polyethylene Compounded Resin HDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified.
Melt Flow 2.0 - 50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
2.0 - 50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Aaron Industries AAROLENE® ARPE LD 300-1 Low Density Polyethylene Compounded Resin
AAROLENE® ARPE 300 Series Polyethylene Compounded Resin LDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified.
Melt Flow 0.30 - 50 g/10 min
<br>@Load 5.00 kg,<br> Temperature 190 °C
0.30 - 50 g/10 min
<br>@Load 11.0 lb,<br> Temperature 374 °F
ASTM D1238
Aaron Industries AVPE HD 300-3 Virgin Polyethylene
Melt flow index may be specified.
Melt Flow 2.0 - 50 g/10 min
<br>@Load 5.00 kg,<br> Temperature 190 °C
2.0 - 50 g/10 min
<br>@Load 11.0 lb,<br> Temperature 374 °F
ASTM D1238
Aaron Industries AVPE LD 300-1 Virgin Polyethylene
Melt flow index may be specified.
Melt Flow 25 - 50 g/10 min
25 - 50 g/10 min
ASTM D1238
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F &nbsp;(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 35 - 50 g/10 min
35 - 50 g/10 min
ASTM D1238
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F &nbsp;(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 30 - 50 g/10 min
30 - 50 g/10 min
ASTM D1238
Polymer Resources PPX-SF1 Modified PPO, Structural Foam Grade, Easy Flow &nbsp;(Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Melt Flow 30 - 50 g/10 min
<br>@Load 21.6 kg,<br> Temperature 170 °C
30 - 50 g/10 min
<br>@Load 47.6 lb,<br> Temperature 338 °F
DDIN 53.735
Lubrizol Advanced Materials Pearlbond® 118 Thermoplastic Polyurethane
The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo..