| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 190 °C |
65
g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
|
Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding
Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection moldi..
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 190 °C |
65
g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
|
Polimeri Europa Riblene® MV 10 R Low Density Polyethylene - Injection Molding
Riblene MV 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 R are highly flexible.Main Applications: Riblene MV 10 R is ideal for injection..
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 210 °C |
65
g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
|
NatureWorks® Ingeo™ 6350D Fiber Grade PLA
NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s..
|
|||
| Melt Flow | 65 g/10 min | 65 g/10 min | 65 cm<sup>3</sup>/10 min; Melt Volume Rate |
|
Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact
Extrusion grade; High microbial resistance, matte surfaceInformation provided by Huntsman
|
|||
| Melt Flow |
65
g/10 min @Load 5.00 kg, Temperature 266 °C |
65
g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
|
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East)
VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries.
|
|||
| Melt Flow |
65
g/10 min @Load 5.00 kg, Temperature 265 °C |
65
g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
|
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati..
|
|||
| Melt Flow |
65
g/10 min @Load 10.0 kg, Temperature 250 °C |
65
g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
|
Samsung Cheil Industries Infino® LH-1070W PC, FR
Information provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
65
g/10 min @Load 1.20 kg, Temperature 300 °C |
65
g/10 min @Load 2.65 lb, Temperature 572 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
|
Chi Mei Wonderlite® PC-175 Polycarbonate
Optical Disk
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg |
65
g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 6.5. |
|
Dow HDPE 65053N High Density Polyethylene
DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellen..
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 230 °C |
65
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Carmel Olefins CAPILENE® SW 75 AV Polypropylene Impact Copolymer
Description: CAPILENE® SW 75 AV is a high melt flow rate, controlled rheology impact copolymer for injection molding. CAPILENE® SW 75 AV is nucleated with antistatic additivation. It is characte..
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 230 °C |
65
g/10 min @Load 4.76 lb, Temperature 446 °F |
|
|
BASF Novolen® 2248 TC Polypropylene
Nucleated grade with antistatic agent for injection moldings.Data was collected by ISO methods and provided by BASF.
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 230 °C |
65
g/10 min @Load 4.76 lb, Temperature 446 °F |
|
|
BASF Novolen® 2348 TC Polypropylene
Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 230 °C |
65
g/10 min @Load 4.76 lb, Temperature 446 °F |
|
|
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 230 °C |
65
g/10 min @Load 4.76 lb, Temperature 446 °F |
|
|
BASF Novolen® 3248 TC Polypropylene
Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 250 °C |
65
g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
|
BASF Ultradur® B 4520 High Speed PBT
Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 275 °C |
65
g/10 min @Load 4.76 lb, Temperature 527 °F |
ISO 1133 |
|
BASF Ultradur B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET |
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 230 °C |
65
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Ineos H65C-00 Polypropylene Homopolymer
This is a high melt flow clarified and lightly lubricated homopolymer designed for high-speed injection molding. It exhibits excellent see-through clarity and meets the requirements of the U.S. Foo..
|
|||
| Melt Flow |
65
g/10 min @Load 10.0 kg, Temperature 250 °C |
65
g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
|
Samsung Cheil Industries Infino® LH-1070W PC, FR
Information provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
65
g/10 min @Load 2.16 kg, Temperature 230 °C |
65
g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
|
Braskem FF650WV Homopolymer Polypropylene
Description: Excellent processability, nucleated.Applications: Suggested uses include fast-cycle injection molding and compounding.Process: Injection Molding.This resin meets the requirements for ol..
|
|||