| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 9.5 g/10 min | 9.5 g/10 min | ASTM D1238 |
|
Multibase Multi-Pro® 2008 X Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
9.5
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
Procedure A Condition L; ASTM D1238 |
|
Network Polymers NPP 25-1011B
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
9.5
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D 1238 |
|
SABIC Innovative Plastics Lexan® FL3000 PC
Structural foam: 10% weight reduction at 0.250" wall with non-brominated and non-chlorinated FR systems. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supp..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
9.5
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
Condition L; ASTM D1238 |
|
PolyMirae Moplen EP648N Injection Molding Grade Polypropylene
Moplen EP648N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP648N is a high gloss block copolymer particularly suitable fo..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
9.5
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D 1238 |
|
SABIC Innovative Plastics Lexan® FL3000 PC (Asia Pacific)
Structural foam: 10% weight reduction at 0.250" wall. ECO-conforming. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supplied by SABIC-IP for the Asia Paci..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 5.00 kg,<br> Temperature 280 °C
|
9.5
g/10 min <br>@Load 11.0 lb,<br> Temperature 536 °F
|
|
|
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Flow, High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts wi..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 5.00 kg,<br> Temperature 280 °C
|
9.5
g/10 min <br>@Load 11.0 lb,<br> Temperature 536 °F
|
|
|
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co..
|
|||
| Melt Flow | 9.5 g/10 min | 9.5 g/10 min | ASTM D1238 |
|
KKPC Kuhmo GP 125EI General Purpose GPPS
Key features: For phonograph, good profile properties. Common Uses: CD-CASE, THIN-WALLGPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding proces..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 2.16 kg,<br> Temperature 250 °C
|
9.5
g/10 min <br>@Load 4.76 lb,<br> Temperature 482 °F
|
ASTM D1238 |
|
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
9.5
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
|
|
Mitsubishi Iupilon® S2000UR 9.5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
9.5
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
|
|
Mitsubishi Iupilon® S2001R 9.5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
9.5
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
|
|
Kraton® D4150 K (SBS) Linear Block Copolymer
Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton..
|
|||
| Melt Flow | 9.5 g/10 min | 9.5 g/10 min | ASTM D1238 |
|
KKPC Kuhmo HI 425TVG High Flow/High Heat Resistant HIPS
Key features: High-impact, High-fluidity Common Uses: TV cover (gas injection).HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between im..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 6.60 kg,<br> Temperature 337 °C
|
9.5
g/10 min <br>@Load 14.6 lb,<br> Temperature 639 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics ULTEM 4001 PEI (Asia Pacific)
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 5.00 kg,<br> Temperature 266 °C
|
9.5
g/10 min <br>@Load 11.0 lb,<br> Temperature 511 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Valox® V2105U PBT
Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio.
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 2.16 kg,<br> Temperature 250 °C
|
9.5
g/10 min <br>@Load 4.76 lb,<br> Temperature 482 °F
|
ASTM D1238 |
|
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled
Good WeatherabilityInformation provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
9.5
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ISO 1133 |
|
Styrolution PS 495F HIPS
Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
9.5
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ISO 1133 |
|
Styrolution PS 495N HIPS
Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
9.5
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ISO 1133 |
|
Styron INSPIREâ„¢ TF1500 ESU Polypropylene
Talc filled, high impact PP compound. INSPIREâ„¢ TF1500 ESU has been developed for aesthetic automotive applications, with good scratch resistance and UV light stabilization.Information provided..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 5.00 kg,<br> Temperature 266 °C
|
9.5
g/10 min <br>@Load 11.0 lb,<br> Temperature 511 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East)
Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio.
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
9.5
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
|
|
Covestro Makrolon® 2803 Polycarbonate, Injection Grade
Medium flowing injection molding grade with UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name ..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
9.5
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
|
|
Covestro Makrolon® 2807 Polycarbonate, Injection Grade
Medium flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
9.5
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
|
|
Covestro Makrolon® 2808 Polycarbonate, Injection Grade
Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
9.5
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
|
|
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 21.6 kg,<br> Temperature 190 °C
|
9.5
g/10 min <br>@Load 47.6 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
ExxonMobil HDPE HTA 001HP2 High Density Polyethylene (HMW) Resin
Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughn..
|
|||
| Melt Flow | 9.5 g/10 min | 9.5 g/10 min | ISO 1133 |
|
Domo 1101M Polypropylene Homopolymer
Information provided by Domo.
|
|||
| Melt Flow |
9.5
-
11.5
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
9.5
-
11.5
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
Arkema Group Orevac® 9307 Y Film EVA-MAH Terpolymer
EVA Terpolymers based Main Applications: Extrusion coating Skin packaging adhesive Thermo-adhesive filmsInformation provided by Arkema Group
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
9.5
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
|
|
Kraton® D4150 K (O/E SBS) Linear Triblock Copolymer
Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton..
|
|||
| Melt Flow |
9.5
g/10 min <br>@Load 2.16 kg,<br> Temperature 235 °C
|
9.5
g/10 min <br>@Load 4.76 lb,<br> Temperature 455 °F
|
ASTM D1238 |
|
Samyang Tribit® 1800H PBT, Extruding Formality
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800H is an extrusion grade.Information pro..
|
|||