Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 9.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Melt Flow 9.5 g/10 min
9.5 g/10 min
ASTM D1238
Multibase Multi-Pro® 2008 X Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Melt Flow 9.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
9.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
Procedure A Condition G; ASTM D1238
Network Polymers F7000 Polystyrene
Description: Ignition RetardantInformation provided by Network Polymers Inc.
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers NPP 25-1011B
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen EP648N Injection Molding Grade Polypropylene
Moplen EP648N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP648N is a high gloss block copolymer particularly suitable fo..
Melt Flow 9.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
9.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co..
Melt Flow 9.5 g/10 min
9.5 g/10 min
ASTM D1238
KKPC Kuhmo GP 125EI General Purpose GPPS
Key features: For phonograph, good profile properties. Common Uses: CD-CASE, THIN-WALLGPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding proces..
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 250 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 482 °F
ASTM D1238
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Melt Flow 9.5 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
9.5 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Mitsubishi Iupilon® S2000R 9.5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Flow 9.5 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
9.5 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Mitsubishi Iupilon® S2000UR 9.5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Flow 9.5 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
9.5 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Mitsubishi Iupilon® S2001R 9.5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
Condition L; ASTM D1238
LyondellBasell Adflexâ„¢ KS311P Polyolefin
Description: Adflexâ„¢ KS-311P thermoplastic olefin resin is a barefoot formulation (no slip, no antiblock) designed for cast film extrusion applications. It is based on proprietary Basell proces..
Melt Flow 9.5 g/10 min
9.5 g/10 min
ASTM D1238
KKPC Kuhmo HI 425TVG High Flow/High Heat Resistant HIPS
Key features: High-impact, High-fluidity Common Uses: TV cover (gas injection).HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between im..
Melt Flow 9.5 g/10 min
<br>@Load 6.60 kg,<br> Temperature 337 °C
9.5 g/10 min
<br>@Load 14.6 lb,<br> Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 4002 PEI
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors.
Melt Flow 9.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
9.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
ISO 1133
Styrolution PS 495F HIPS
Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection..
Melt Flow 9.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
9.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
ISO 1133
Styrolution PS 495N HIPS
Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor..
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Styron INSPIREâ„¢ TF1500 ESU Polypropylene
Talc filled, high impact PP compound. INSPIREâ„¢ TF1500 ESU has been developed for aesthetic automotive applications, with good scratch resistance and UV light stabilization.Information provided..
Melt Flow 9.5 g/10 min
<br>@Load 3.80 kg,<br> Temperature 230 °C
9.5 g/10 min
<br>@Load 8.38 lb,<br> Temperature 446 °F
ASTM Data
Styron Magnumâ„¢ 4455 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 250 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled
Good WeatherabilityInformation provided by Samsung Cheil Industries.
Melt Flow 9.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
9.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS
Melt Flow 9.5 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
9.5 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Covestro Makrolon® 2807 Polycarbonate, Injection Grade
Medium flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially..
Melt Flow 9.5 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
9.5 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Covestro Makrolon® 6465 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici..
Melt Flow 9.5 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
9.5 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Covestro Makrolon® 6485 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was ..
Melt Flow 9.5 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
9.5 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Covestro Makrolon® 6557 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding grade with easy mold release, UV-stabilized.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer A..
Melt Flow 9.5 g/10 min
<br>@Load 21.6 kg,<br> Temperature 190 °C
9.5 g/10 min
<br>@Load 47.6 lb,<br> Temperature 374 °F
ASTM D1238
ExxonMobil HDPE HTA 001HP2 High Density Polyethylene (HMW) Resin
Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughn..
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin
Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un..
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 275 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 527 °F
Arkema Group Orgalloy® RS 66M25 Nylon 66 Alloy, 25% Mineral Filled (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ISO 1133
Barlog Plastics KEBAFORM C 901 SO POM Copolymer unreinforced, improved wear and friction
POMInformation provided by BARLOG plastics GmbH.
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Carmel Olefins CAPILENE® QM 45 F Propylene Random Copolymer
Description: CAPILENE® QM 45 F is a slip and anti-block formulated random copolymer. It is characterized by high gloss and easy processing.Applications: CAPILENE® QM 45 F is suitable for cast u..
Melt Flow 9.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
9.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
Kraton® D4150 K (O/E SBS) Linear Triblock Copolymer
Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton..
Melt Flow 9.5 g/10 min
<br>@Load 2.16 kg,<br> Temperature 235 °C
9.5 g/10 min
<br>@Load 4.76 lb,<br> Temperature 455 °F
ASTM D1238
Samyang Tribit® 1800H PBT, Extruding Formality
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800H is an extrusion grade.Information pro..
Copyright © lookpolymers.com All Rights Reserved