| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 12.7 - 76.0 microns | 0.500 - 2.99 mil | Recommended range for processing |
|
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without ..
|
|||
| Thickness | 12.7 - 140 microns | 0.500 - 5.50 mil | Average value: 63.0 microns Grade Count:24 |
|
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Adhesive |
|
Dielectric Polymers NT4500 Protective Film
(discontinued **)
Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA..
|
|||
| Thickness | 12.7 microns | 0.500 mil | |
|
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es..
|
|||
| Thickness | 12.7 - 127 microns | 0.500 - 5.00 mil | Recommended range for processing |
|
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
|
|||
| Thickness | 12.7 - 10000 microns | 0.500 - 394 mil | Average value: 1440 microns Grade Count:15 |
|
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
|
|||
| Thickness | 12.7 microns | 0.500 mil | 4:1 BUR; Neck Height = 8 Die Diameters |
|
LyondellBasell Alathon® L4907 High Density Polyethylene
ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Nominal; ExxonMobil Method |
|
ExxonMobil Bicor® 50 LBW OPP Film
Product Description: Bicor LBW is a two-sided treated, slip modified, non-heat sealable OPP film designed for use as the outside web of a lamination. The print surface is treated and can be printed ..
|
|||
| Thickness | 12.7 microns | 0.500 mil | |
|
ExxonMobil Label-Lyte® 612 LLG-102 Clear OPP Film
Clear, polypropylene films designed for use in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. The print surface is a treated high ene..
|
|||
| Thickness | 12.7 microns | 0.500 mil | ExxonMobil Method |
|
ExxonMobil Label-Lyte™ 612LLG102 OPP Film
Product Description: A clear, two-side treated, polypropylene film that is used in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. 612..
|
|||
| Thickness | 12.7 microns | 0.500 mil | ExxonMobil Method |
|
ExxonMobil Metallyte™ 12MM281 OPP Film
Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. 12MM281 is designed for use as the center web of a triplex adhesive lamination. The treated s..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 444 Double Coated Tapes with Adhesive 300
3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Side 1, Skim Coat |
|
Arlon 55578XC028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 9737 Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 9741R Double Coated Tape
3M™ Double Coated Tape 9741 is a 6.5 mil double coated tape utilizing a 0.5 mil hand-tearable polyester film heavily coated on both sides with 3 mils of an ultra high peel acrylic adhesive system. ..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 9828PC Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Side 2 |
|
Arlon R33073X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 7628 FiberglassSide 2: Cured Silicone RubberInterleave: NoneThis data represents typical values for the production material and should ..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Facestock |
|
3M FM002 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Facestock |
|
3M FM00N Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Side 2 |
|
Arlon 51163X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber50" wideThis data represents typical values for the production material and should not..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Polyester |
|
3M 7953MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Side 1, Skim Coat |
|
Arlon 55578XA030M 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 9019 Double Coated Tapes with Adhesive 300
3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 9828HL Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 9629FL Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
|
|||
| Thickness | 12.7 microns | 0.500 mil | Carrier |
|
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
|
|||
| Thickness | 12.7 microns | 0.500 mil | |
|
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness...
|
|||
| Thickness | 12.7 microns | 0.500 mil | |
|
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness...
|
|||
| Thickness | 12.7 microns | 0.500 mil | |
|
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness...
|
|||