| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 25.0 - 80.0 microns | 0.984 - 3.15 mil | Recommended |
|
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Premix Thermoplastics PREFLEX E25 Polyphenylene Ether (PPO/PPE)
PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material ..
|
|||
| Thickness | >= 25.0 microns | >= 0.984 mil | |
|
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin
Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin
FP019-D is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Slip, Antiblock, Polymer Process AidApplications: Hig..
|
|||
| Thickness | 25.0 microns | 0.984 mil | As tested for properties on this data sheet |
|
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film
FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
|
|||
| Thickness | 25.0 - 150 microns | 0.984 - 5.91 mil | Recommended range for processing |
|
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film
FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **)
Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Total Finathene® LL 6010 FH 18P LLDPE film
(discontinued **)
Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Formosa Plastics Formolene® FORMAX® L71709A Film (Hexene Grade) LLDPE
(discontinued **)
High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Formosa Plastics Formolene® FORMAX® L71709H Film (Hexene Grade) LLDPE
(discontinued **)
High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Formosa Plastics Formolene® FORMAX® L91507E2 Film (Hexene Grade) LLDPE
(discontinued **)
Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. ..
|
|||
| Thickness | 25.0 microns | 0.984 mil | extruded at 2:1 BUR |
|
Lotte Chemical Titan TITANEX® LF2021 Linear low density polyethylene resin
(discontinued **)
LF2021 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown and cast film extrusion which offers outstandin..
|
|||
| Thickness | 25.0 - 75.0 microns | 0.984 - 2.95 mil | Recommended range for processing |
|
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin
HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Braskem Flexus® 9210 LLDPE Blown Film Extrusion
(discontinued **)
25µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); multilayer packaging films; films for lamination. Information provided by Braskem
|
|||
| Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
|
Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 25 µm)
HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has co..
|
|||
| Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
|
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co..
|
|||
| Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
|
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm)
LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron..
|
|||
| Thickness | 25.0 microns | 0.984 mil | As Tested |
|
Solvay Specialty Polymers Ajediumâ„¢ PVDF 9009 Polyvinylidene Fluoride (PVDF)
Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Shandong Dongyue Shenzhou New Material Co CHFM 025 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
UBE 5034C2 NCH Nylon 6/66 Film
Description: T-die cast film of 25µm in thicknessInformation provided by UBE.
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Formosa Plastics Formolene® L42009A Film (Butene Grade) LLDPE
Butene Copolymer (High Antiblock)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration a..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE
Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food ..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of ..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high ..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Braskem BF0323/12HC Blown Film Extrusion Low Density Polyethylene
Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem.
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Formosa Plastics Formolene® L62608PA Film (Hexene Grade) LLDPE
(discontinued **)
Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he..
|
|||