Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 1.97 mil Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Thickness 50.0 - 250 microns
1.97 - 9.84 mil
Recommended
Polimeri Europa Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 20 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 20 is characterized by a high melt strength leading to a good bubble sta..
Thickness 50.0 - 250 microns
1.97 - 9.84 mil
Recommended
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le..
Thickness 50.0 microns
1.97 mil
Recommended
Parker Chomerics CHO-SHIELD® 610 A/B Epoxy Conductive Coating
Description: CHO-SHIELD® 610 A/B is a highly conductive, two-component silver-plated-copper filled epoxy coating for application to non-conductive plastic substrates, particularly those subject to ..
Thickness >= 50.0 microns
>= 1.97 mil
Bondline thickness
Parker Chomerics THERM-A-GAP™ GEL 8010 High Performance Fully Cured Dispensable Gel
Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) compl..
Thickness 50.0 microns
1.97 mil
PSA Thickness; Visual
Parker Chomerics T-Wings Heat Spreaders
Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade..
Thickness 50.0 microns
1.97 mil
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film
The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng..
Thickness 50.0 microns
1.97 mil
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging
The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th..
Thickness 50.0 microns
1.97 mil
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging
The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength..
Thickness 50.0 - 200 microns
1.97 - 7.87 mil
Recommended
Polimeri Europa Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 50 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FD 50 exhibit good optical and sealing properties, high flexibility and toughnes..
Thickness 50.0 microns
1.97 mil
SABIC HP0722N Low Density Polyethylene for Blown Film
Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti..
Thickness 50.0 microns
1.97 mil
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film
The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing ..
Thickness 50.0 microns
1.97 mil
± 2.5%; ASTM-252-78
Kinlead PG12 Bag Grade BOPP Plain Film (thickness: 50 µm)
PG12 is a high slippery and low static, bag grade BOPP plain film. It is transparent and non heat sealable. One side has corona treatment. It is widely used in gift wrapping and textiles with high s..
Thickness 50.0 microns
1.97 mil
± 2.5%; ASTM-252-78
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 50 µm)
PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an..
Thickness 50.0 microns
1.97 mil
extruded at 2.5:1 BUR
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene
LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Thickness 50.0 microns
1.97 mil
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
Thickness 50.0 microns
1.97 mil
Total PPH 6088 Polypropylene Homopolymer, Cast Film
Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH..
Thickness 50.0 microns
1.97 mil
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade
Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld..
Thickness 50.0 microns
1.97 mil
film
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Thickness 50.0 microns
1.97 mil
film
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
Thickness 50.0 microns
1.97 mil
film
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
Thickness 50.0 microns
1.97 mil
film
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Thickness 50.0 microns
1.97 mil
Braskem TS9022 Blown Film Extrusion Low Density Polyethylene
Films for automatic overwrap packaging of hygiene markets. Typical applications are toilet tissue, kitchen paper and napkin (paper product) overwrap. Films which require good optical properties al..
Thickness 50.0 microns
1.97 mil
Carmel Olefins IPETHENE® 113 Low Density Polyethylene
IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Thickness 50.0 microns
1.97 mil
Carmel Olefins IPETHENE® 323 Low Density Polyethylene
IPETHENE® 323 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Thickness 50.0 microns
1.97 mil
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade
The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,..
Thickness 50.0 microns
1.97 mil
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film
The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc..
Copyright © lookpolymers.com All Rights Reserved