| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 127 microns | 5.00 mil | cured, per ply |
|
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
|
|||
| Thickness | 127 microns | 5.00 mil | Backing |
|
Dielectric Polymers NT-500 Protective Film
(discontinued **)
Crosslinked silicone adhesive with electrical grade polyester film backing.Features: Clean tape removalNo film shrinkage after exposure to elevated temperaturesApplications: Used as a fume mask duri..
|
|||
| Thickness | 127 microns | 5.00 mil | Nominal |
|
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
|
|||
| Thickness | 127 microns | 5.00 mil | Nominal |
|
DuPont™ Nomex® E56 Paper, 5 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
|
|||
| Thickness | 127 microns | 5.00 mil | Tape Only |
|
3M 1026 Adhesive Transfer Tape
3M™ Adhesive Transfer Tape 1026 is a 300 high strength acrylic adhesive on a 4 mil liner. Adhesive transfer tape in a pre-cut, tape strip on a pad.Features:5.0 mil adhesive transfer tape on a pad. ..
|
|||
| Thickness | 127 microns | 5.00 mil | Total; ASTM D3652 |
|
3M 3294 Vent Tape
3M™ Vent Tape 394 is a non-woven, synthetic backing with a strip-coated low-tack pressure sensitive adhesive for use in various venting applications requiring high outgassing rates.Information prov..
|
|||
| Thickness | 127 - 178 microns | 5.00 - 7.00 mil | Side 2 |
|
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: 0.005" FEP FilmThis data represents typical values for the production material and should not be used as ..
|
|||
| Thickness | 127 microns | 5.00 mil | Carrier; Arlon SQA-TMS-003 |
|
Arlon 32580R020 0.020" (0.508 mm) Uncured Silicone Rubber on Polyester Film Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmAppearance: Red silicone gum on polymer linerThis data represents typical values for the production..
|
|||
| Thickness | 127 microns | 5.00 mil | Carrier; Arlon SQA-TMS-003 |
|
Arlon 32980XA015 0.015" Uncured Silicone Rubber on Polyester Film
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as ..
|
|||
| Thickness | 127 microns | 5.00 mil | Adhesive |
|
3M 9672LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate |
|
Arlon R32390B020 0.020" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassAll ingredients of product are listed in 21 CFR 177.26000This data represe..
|
|||
| Thickness | >= 127 microns | >= 5.00 mil | Side 2 |
|
Arlon R34696R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Thickness | 127 microns | 5.00 mil | Facestock |
|
3M FL015 Lexan Label Product
3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high ..
|
|||
| Thickness | 127 microns | 5.00 mil | Tape |
|
3M XP2112 Hi-Performance Adhesive Transfer Tape
3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of..
|
|||
| Thickness | 127 microns | 5.00 mil | Backing; ASTM D3752 |
|
3M 398FR Glass Cloth Tape
3M™ Glass Cloth Tape 398FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typically used for se..
|
|||
| Thickness | 127 microns | 5.00 mil | Prime Coated 1165 Fiberglass, Substrate |
|
Arlon 44571B010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place..
|
|||
| Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 1 |
|
Arlon 51571R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum on fiberglass clothThis data Represents typical values for the production material. ..
|
|||
| Thickness | 127 microns | 5.00 mil | Side 1; Arlon SQA-TMS-003 |
|
Arlon 55102R024 0.024" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.In..
|
|||
| Thickness | 127 microns | 5.00 mil | Polyester |
|
3M 7959MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
|
|||
| Thickness | 127 microns | 5.00 mil | Poly, Interleave |
|
Arlon R34880T020 0.020" (0.508 mm) Uncatalyzed, Unsupported rubber on a Mylar Carrier
Design/Construction:Side 1: Uncatalyzed, Unsupported rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, ..
|
|||
| Thickness | 127 microns | 5.00 mil | Facestock |
|
3M FL019 Lexan Label Product
3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high ..
|
|||
| Thickness | 127 microns | 5.00 mil | Adhesive |
|
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
|
|||
| Thickness | 127 - 635 microns | 5.00 - 25.0 mil | |
|
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet
(discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
|
|||
| Thickness | 127 - 635 microns | 5.00 - 25.0 mil | |
|
Alcoa KAMA 1200 Utility Clear OPS, Sheet
(discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
|
|||
| Thickness | 127 microns | 5.00 mil | Polyester Film Carrier; Arlon SQA-TMS-003 |
|
Arlon 32980R015 0.015" (0.381 mm) Uncured Silicon Rubber on Polyester Film Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmProduct Use: Flexible heater substrateAppearance: Red colored, high viscosity gum on polymer liners..
|
|||
| Thickness | >= 127 microns | >= 5.00 mil | Side 1 |
|
Arlon 44560R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
|
|||
| Thickness | 127 microns | 5.00 mil | Prime Coated 1165 Fiberglass, Substrate |
|
Arlon 44570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use..
|
|||
| Thickness | 127 - 165 microns | 5.00 - 6.50 mil | Overall |
|
Arlon 48571R006 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif..
|
|||
| Thickness | 127 microns | 5.00 mil | Carrier; Arlon SQA-TMS-003 |
|
Arlon R37503G060 0.060" Uncured Fluorosilicone on Release PET Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured FluorosiliconeCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be used ..
|
|||