Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 13.0 microns Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Thickness 13.0 microns
0.512 mil
printed through a 230 mesh SS screen with 13 micron emulsion back off
Gwent Electronic Materials C10903P14 Carbon/Graphite Ink
Carbon Graphite Ink is used for screen printing working electrodes. This is a carbon graphite ink, which has been optimized to give superior electrochemical performance with good reversibility when..
Thickness 13.0 microns
0.512 mil
Cured, Typical, Using a 156 mesh stainless steel screen, 13 micron emulsion
Gwent Electronic Materials C2090225D7 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
Thickness 13.0 microns
0.512 mil
when printed through a 156 mesh
Gwent Electronic Materials C61003P7 Silver / Silver Chloride Paste
C61003P7 has a ratio of Silver to Silver Chloride of 60/40. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a fa..
Thickness 13.0 - 15.0 microns
0.512 - 0.591 mil
Gauge
UBE 1024FDX41 Nylon 6 BOPA Film
Specialties: Excellent processing stabilityProcessing: Best for BOPAApplications: BOPA film (T-die)Information provided by UBE.
Thickness 13.0 microns
0.512 mil
Dow LDPE 752A Low Density Polyethylene, Film Grade
DOW LDPE 752A resin is a drawdown film resin for thin gauge applications such as garment films. It contains high levels of both slip and antiblock additives. This material complies with U.S.FDA regu..
Thickness 13.0 microns
0.512 mil
Upward surface, as processed; Mitutoyo Surftest-402
3D Systems CastForm™ PS Plastic for SLS® Systems
For use with all selective laser sintering (SLS®) systems.ApplicationsCreate patterns directly rather than through indirect methodsComplex investment casting patternsReactive metals like titaniumLo..
Copyright © lookpolymers.com All Rights Reserved