| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 150 microns | 5.91 mil | extruded at 1.5:1 BUR |
|
Lotte Chemical Titan TITANLENE® LDF265YZ Low density polyethylene
LDF265YZ is a low density polyethylene resin for film extrusion. LDF265YZ has no slip and anti-block additives. LDF265YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
|
|||
| Thickness | 150 microns | 5.91 mil | |
|
Isoflon Tisoflon® 5K Polytetrafluoroethylene Coated Kevlar Fabric
PTFE coated Kevlar fabric TISOFLON®Information provided by Isoflon.
|
|||
| Thickness | 150 microns | 5.91 mil | extruded at 1.5:1 BUR |
|
Lotte Chemical Titan TITANLENE® LDF264YZ Low density polyethylene
LDF264YZ is a low density polyethylene resin for film extrusion. LDF264YZ has no slip and anti-block additives. LDF264YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
|
|||
| Thickness | 150 - 1500 microns | 5.90 - 59.0 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.2 |
|
Sinotek Materials B Graphite Roll
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FM01961K MC Polyester Label Products
3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FM05540K MC Polyester Label Products
3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FM118K Indoor UL Recognized MC Polyester Label Products
3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FM16K Indoor UL Recognized Computer Imprintable White Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FV100K Soft White Vinyl EDP Label Product
3M™ Soft White Vinyl EDP Label Products FV100K and FV1002 are flexible vinyl label stocks that offer excellent durability and some moisture resistance. These vinyl labels utilize 3M™ Adhesive F220..
|
|||
| Thickness | 150 microns | 5.90 mil | Total Thickness |
|
3M 92015 Double Coated Tape with Adhesive 200MP
3M™ Double Coated Tapes with 3M™ Adhesive 200MP feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. The 3M adhesive 200MP provide..
|
|||
| Thickness | 150 microns | 5.90 mil | Total Thickness |
|
3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FM14K Indoor UL Recognized Computer Imprintable Clear Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FM02511K Clear Laser Imprintable Label Product
3M™ Clear Laser Imprintable Label Product FM02511K is a durable high performance material that offers excellent thermal stability and moisture resistance. This product is suitable for demanding app..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FM03K Indoor UL Recognized Clear Polyester Label Products
on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem..
|
|||
| Thickness | 150 microns | 5.90 mil | Liner |
|
3M FM04630K White Polyester Label Product
3M™ White Polyester Label Products FM046302 and FM04630K are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Ad..
|
|||
| Thickness | 150 microns | 5.91 mil | |
|
Shandong Dongyue Shenzhou New Material Co CHFM 150 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
|
|||
| Thickness | 150 - 1500 microns | 5.90 - 59.0 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.1 |
|
Sinotek Materials A Graphite Roll
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Thickness | 150 - 1500 microns | 5.90 - 59.0 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.3 |
|
Sinotek Materials C Graphite Roll
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Thickness | 150 - 1500 microns | 5.90 - 59.0 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.4 |
|
Sinotek Materials D Graphite Roll
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||