| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 180 - 1020 microns | 7.09 - 40.2 mil | |
|
Parker Chomerics CHO-BOND® 1016 Electrically Conductive Sealant
Description: CHO-BOND 1016 sealant is an electrically conductive, one-component RTV silicone which provides both environmental sealing and EMI shielding. This seal, filled with nickel-plated graphit..
|
|||
| Thickness | 180 - 12700 microns | 7.09 - 500 mil | |
|
Parker Chomerics Duralan II™ AR Polycarbonate Unshielded Window
Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate. A unique feature of Parker Chomerics window products is the capability..
|
|||
| Thickness | 180 - 12700 microns | 7.09 - 500 mil | |
|
Parker Chomerics Duralan II™ P Polycarbonate Unshielded Window
Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate. A unique feature of Parker Chomerics window products is the capability..
|
|||
| Thickness | 180 - 12700 microns | 7.09 - 500 mil | Average value: 4290 microns Grade Count:5 |
|
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
|
|||
| Thickness | 180 microns | 7.09 mil | |
|
Isoflon Tisoflon® 6S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
|
|||
| Thickness | 180 microns | 7.10 mil | |
|
Hexcel® HexForce™ 1035 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
|
|||
| Thickness | 180 microns | 7.10 mil | Total |
|
3M 470 Electroplating Tape
3M™ Electroplating Tape 470 is a conformable and abrasion-resistant vinyl tape with excellent resistance to most chemicals used in typical electroplating processes.Information provided by 3M
|
|||
| Thickness | 180 microns | 7.10 mil | Total |
|
3M 470L Electroplating Tape
3M™ Electroplating Tape 470L is a linered version of 3M vinyl tape 470 that may be used for die-cutting or large area applications.Information provided by 3M
|
|||