| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | >= 25.0 microns | >= 0.984 mil | |
|
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo..
|
|||
| Thickness | >= 25.0 microns | >= 0.984 mil | |
|
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin
Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **)
Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Formosa Plastics Formolene® FORMAX® L91507A Film (Hexene Grade) LLDPE
(discontinued **)
Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. ..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Formosa Plastics Formolene® FORMAX® L91507H Film (Hexene Grade) LLDPE
(discontinued **)
Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. ..
|
|||
| Thickness | 25.0 microns | 0.984 mil | extruded at 2:1 BUR |
|
Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin
(discontinued **)
LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughne..
|
|||
| Thickness | 25.0 microns | 0.984 mil | extruded at 2:1 BUR |
|
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin
(discontinued **)
LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down..
|
|||
| Thickness | 25.0 microns | 0.984 mil | extruded at 2.5:1 BUR |
|
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin
(discontinued **)
Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile..
|
|||
| Thickness | 25.0 microns | 0.984 mil | extruded at 2.5:1 BUR |
|
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin
(discontinued **)
Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre..
|
|||
| Thickness | 25.0 microns | 0.984 mil | extruded at 2.5:1 BUR |
|
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin
(discontinued **)
Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin
PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur..
|
|||
| Thickness | 25.0 - 75.0 microns | 0.984 - 2.95 mil | Recommended range for processing |
|
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin
HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che..
|
|||
| Thickness | 25.0 - 75.0 microns | 0.984 - 2.95 mil | |
|
NOVA Chemicals Sclair® 14L1 Octene LMDPE Film Resin
(discontinued **)
Low gel, Good clarity, Excellent sealing characteristicsApplications: Lamination, Co-extrusionAdditives: Process stabilizer, polymer process aidFilm properties are typical of blown film extruded at ..
|
|||
| Thickness | 25.0 microns | 0.984 mil | As tested |
|
Metabolix M-veraâ„¢ B5010 Film Grade Compostable Bioplastic
For use in tough, certified compostable film and bag applications. Mvera B5010 offers a wide range of attractive traits—excellent tear and puncture toughness, excellent seal strength, good prin..
|
|||
| Thickness | 25.0 microns | 0.984 mil | Using a 156 mesh stainless steel screen, 13 micron emulsion |
|
Gwent Electronic Materials C2080409D2 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 85/15. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
|
|||
| Thickness | 25.0 - 36.0 microns | 0.984 - 1.42 mil | Cured, Printed through 230 stainless steel mesh with 13 micron emulsion |
|
Gwent Electronic Materials C2100126D6 Carbon Graphite Ink
This ink is designed for biosensor applications, it gives a good electrochemical response when tested with buffered Ferricyanide solutions. This product is based on a unique curing process that resu..
|
|||
| Thickness | 25.0 microns | 0.984 mil | As Tested |
|
Solvay Specialty Polymers Ajediumâ„¢ KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Shandong Dongyue Shenzhou New Material Co CHFM 025 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
UBE 1022C2 NCH Nylon 6 Film
Description: T-die cast film of 25µm in thicknessInformation provided by UBE.
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow ATTANE™ 4301 Ultra Low Density Polyethylene, Blown Film Grade
ATTANE® 4301 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It has low levels of sli..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade
ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow ATTANE™ 4601 Ultra Low Density Polyethylene, Medical Packaging Grade
ATTANE® 4601 copolymer is an ultra low density polyethylene blown film extrusion grade having high impact resistance and tear strength combined with improved softness, designed for use in medical p..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Braskem F2022/0 Cast Film Extrusion Low Density Polyethylene
Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem.
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene
Description: LH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount.Applications: Lamina..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount. The minimum biobas..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process..
|
|||
| Thickness | 25.0 microns | 0.984 mil | |
|
NOVA Chemicals Surpass® FPs117-D Octene sLLDPE Film Resin
(discontinued **)