Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 3.20 mil Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Thickness 81.3 microns
3.20 mil
2 oz. Total Tickness; ASTM D1000
Parker Chomerics CHO-MASK II ST Conductive Foil Tape
The CHO-MASK II family of EMI foil tapes includes both Standard Tack (ST) and High Tack (HT) versions for providing a conductive, non-corroding surface on painted metal electronic enclosures. CHO-MA..
Thickness 81.3 microns
3.20 mil
Hexcel® HexForce™ 1620 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 81.3 microns
3.20 mil
Liner
3M 7000FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Thickness 81.3 microns
3.20 mil
Liner
3M 7002FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Thickness 81.3 microns
3.20 mil
Liner
3M 7777 Polypropylene Label Material
3M™ Polypropylene Label Material 7777 is a durable material that offers good thermal stability and moisture resistance. This label material utilizes 3M™ Permanent Acrylic Adhesive, which is design..
Thickness 81.3 microns
3.20 mil
Liner
3M 9447 Adhesive Transfer Tape
3M™ Adhesive Transfer Tape 9447 is specifically designed for use with 3M™ Label Component Systems for protected graphics printing of polyester films. Also can be used in constructing custom tamper..
Thickness 81.3 microns
3.20 mil
Backside Adhesive
3M 9456 Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
Thickness 81.3 microns
3.20 mil
Liner
3M 9458 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Thickness 81.3 microns
3.20 mil
Liner Caliper
3M 9824 Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
Thickness 81.3 microns
3.20 mil
Liner
3M FV292 White Vinyl Label Products
3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14..
Thickness 81.3 microns
3.20 mil
Facestock
3M PS195 White Yupo™ TIS Label Products
3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g..
Thickness 81.3 - 152 microns
3.20 - 6.00 mil
Dry
3M Scotchkote™ EA5WB WB Epoxy Coating
3M Scotchkote WB Epoxy Coating EA5WB is a member of the expanding range of 3M Scotchkote high performance coating. It has been specifically developed for original equipment manufacture, particularly..
Thickness 81.3 microns
3.20 mil
Liner
3M 7603 Clear Vinyl Label Material
3M™ Clear Vinyl Label Material 7603 is a soft, flexible vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick tack an..
Thickness 81.3 microns
3.20 mil
Liner
3M 7847 Laser Markable Label Material
3M™ Laser Markable Label Material 7847 and 7848 are specialty film label materials where a laser can ablate the top layer of a dual-layer facestock to create an image. The same laser can also kiss ..
Thickness 81.3 microns
3.20 mil
Liner
3M 7880 Computer-Imprintable Polyester Label Material
3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional..
Thickness 81.3 microns
3.20 mil
Liner
3M 7883 Computer-Imprintable Polyester Label Material
3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition..
Thickness 81.3 microns
3.20 mil
Release Liner
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Thickness 81.3 microns
3.20 mil
Release Liner
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Thickness 81.3 microns
3.20 mil
Liner
3M 7840 Laser Toner Printable Polyester Label Material
3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi..
Thickness 81.3 microns
3.20 mil
Total; ASTM D3752
3M 8992L Polyester Tape
3M™ Polyester Tape 8992L is a dark green polyester tape with silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and ba..
Thickness 81.3 microns
3.20 mil
Caliper
3M 9593 Double Coated Tapes with Adhesive 350
3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a ..