Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 3.50 mil Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Thickness 88.9 microns
3.50 mil
Backing
Dielectric Polymers NT-988-2 Overlap Splice Tape  (discontinued **)
Acrylic copolymer adhesive with silicone treated release paper backing.Features: Chemical resistantGood conformabilityPlasticizer migration resistantExcellent adhesion to low surface energy substrat..
Thickness 88.9 microns
3.50 mil
Silicone release coated kraft liner
Dielectric Polymers NT-490 Polyimide Label Stock  (discontinued **)
High temperature acrylic adhesive with thermal transfer imprintable polyimide film backing.Features: Meets ANSI standards for print contract signals and minimum reflectance ratios for bar code print..
Thickness 88.9 microns
3.50 mil
Hexcel® HexForce™ 220HT Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 88.9 microns
3.50 mil
Total
3M 1125 EMI Shielding Tape
3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by..
Thickness >= 88.9 microns
>= 3.50 mil
Side 2
Arlon 28571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
Thickness 88.9 microns
3.50 mil
Side 1
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat..
Thickness 88.9 microns
3.50 mil
Side 2; Arlon SQA-TMS-003
Arlon 51576R015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate..
Thickness 88.9 microns
3.50 mil
Side 1; Arlon SQA-TMS-003
Arlon 51576XC15A 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PolyethyleneSide 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the producti..
Thickness 88.9 microns
3.50 mil
Side 2, Layer 2; Arlon SQA-TMS-003
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc..
Thickness 88.9 microns
3.50 mil
Liner
3M 9471 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Thickness 88.9 microns
3.50 mil
Tape
3M 9737 Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
Thickness 88.9 microns
3.50 mil
Total (excluding liner)
3M 9740 Double Coated Tape
3M™ Double Coated Tape 9740 is a 3.5 mil double coated tape utilizing a 0.5 mil (12 microns) polyester film coated on both sides with 1.5 mils (38 microns) of a high shear acrylic adhesive system. ..
Thickness 88.9 microns
3.50 mil
Layer 1; Arlon SQA-TMS-003
Arlon 55869R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV03S Indoor UL Recognized White Vinyl Label Products
3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV06B Semi-Rigid White Vinyl Label Product
3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV09D Soft Translucent Vinyl Label Products
3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV1172 Removable White Vinyl Label Products
3M™ Removable White Vinyl Label Products FV1172 and FV392 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive ..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV1225 Removable Vinyl Label Products
3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV172 Soft Translucent Vinyl Label Products
3M™ Soft Translucent Vinyl Label Products FV172 and FV173 are flexible, conformable matte clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adh..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV233 Soft Yellow Vinyl Label Products
3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV362 Soft Yellow Vinyl Label Products
3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar..
Thickness 88.9 microns
3.50 mil
Facestock
3M FVT40 Tire Label Product
3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress..
Thickness 88.9 microns
3.50 mil
Prime Coated 2113 Fiberglass, Substrate
Arlon 47576R009 0.0095" (0.241 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data sho..
Thickness 88.9 microns
3.50 mil
Side 2; Arlon SQA-TMS-003
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti..
Thickness 88.9 microns
3.50 mil
Side 2
Arlon 51561R015 0.015" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the ..
Thickness 88.9 microns
3.50 mil
Side 2; Arlon SQA-TMS-003
Arlon 51576R015D 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical v..
Thickness 88.9 microns
3.50 mil
Adhesive
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS..
Thickness 88.9 microns
3.50 mil
Facestock
3M FV023202 White Vinyl Label Products
3M™ White Vinyl Label Products are flexible and conformable materials that offer durability and moisture resistance. The polymerically plasticized nature of this soft vinyl imparts long term dimens..
Thickness 88.9 microns
3.50 mil
Liner
Dielectric Polymers NT-988 High Tack Laminating Adhesive  (discontinued **)
Acrylic copolymer adhesive with silicone treated release paper liner.Features: Excellent adhesion to low surface energy substratesCompatible with most printing inksApplications: Mounting a wide vari..
Thickness 88.9 microns
3.50 mil
Prime Coated 2113 Fiberglass, Substrate
Arlon 47573R007 0.0075" (0.190 mm) Cured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured RubberSide 2: Cured Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifica..
Copyright © lookpolymers.com All Rights Reserved