| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 1020 microns | 40.0 mil | |
|
Zircar Refractory Composites SIL-3 Silica Cloth
ZIRCAR Type SIL Silica Cloths consists of high temperature non textured amorphous silica fiber yarn, woven into an extremely strong fabrics. These non preshrunk textiles are ideal for applications ..
|
|||
| Thickness | 1020 microns | 40.0 mil | |
|
Daikin NEOFLON NF-1000 FEP Film
NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el..
|
|||
| Thickness | 1020 microns | 40.0 mil | Tape |
|
3M 1640 Cylinder Mount Build-Up Tape
3M™ Cylinder Mount Build-Up Tape 1640 is a non-compressible vinyl carrier coated on one side with a pressure sensitive acrylic adhesive designed for building-up print cylinder diameter to help meet..
|
|||
| Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 32570R040 0.040" (1.02 mm) Uncured Silicone Rubber with Fiberglass Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be use..
|
|||
| Thickness | 1020 microns | 40.0 mil | Side 1; Arlon SQA-TMS-003 |
|
Arlon 32570R040 0.040" (1.02 mm) Uncured Silicone Rubber with Fiberglass Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be use..
|
|||
| Thickness | 1020 microns | 40.0 mil | Side 2; Arlon SQA-TMS-003 |
|
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene..
|
|||
| Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 55146R040 0.040"(1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil..
|
|||
| Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 61089R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Denier Vectran HS Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 1000 Denier HS Appearance: Red silicone gum on fabricThis data represents t..
|
|||
| Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 940-15R##-P0 0.040" (1.02 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1.5” Wide Rectangular 1.5 inch wide, 40 mil thick, Red, Rectangular cross-section, Self-f..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
|
Arlon HSLW401R##-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: High Strength, 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-012 |
|
Arlon LW40125B12-P0 0.040" Self-Fusing Silicone Rubber Tape
1.25 inches wide, 40 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in 12 yard long roll lengths.Design/Construction:Rubber: Cured Self-fusing Silicone R..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
|
Arlon LW401A##-P3 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Blue, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length ..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
|
Arlon LW401B##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
|
Arlon LW401B##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
|
Arlon LW401C##FR-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
|
Arlon LW401R##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
|
Arlon LW401R##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-003 |
|
Arlon LW401Y##-M1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Yellow, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll lengt..
|
|||
| Thickness | 1020 microns | 40.0 mil | Dry |
|
3M Scotchkote™ UV 840 Urethane Coating
Scotchkote Urethane Coating UV 840 has been developed to provide a durable gloss finish for use as the final coat of 3M coating systems in the construction and transport industries, where an ease of..
|
|||
| Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material..
|
|||
| Thickness | 1020 microns | 40.0 mil | Side 1; Arlon SQA-TMS-003 |
|
Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material..
|
|||
| Thickness | 1020 microns | 40.0 mil | Total |
|
3M 4411B Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
|
|||
| Thickness | 1020 microns | 40.0 mil | Total |
|
3M 4411G Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
|
|||
| Thickness | 1020 microns | 40.0 mil | Total |
|
3M 4411N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
|
|||
| Thickness | 1020 microns | 40.0 mil | overall; Arlon SQA-TMS-003 |
|
Arlon 49283R040 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber
|
|||
| Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 55586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEAppearance: Red silicone gum and rubber on fiberglass clothThis data ..
|
|||
| Thickness | 1020 microns | 40.0 mil | Rubber; Arlon SQA-TMS-012 |
|
Arlon RBLW401X##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths. ## in the product number indicates roll length in yards..
|
|||
| Thickness | 1020 microns | 40.0 mil | Overall; Arlon SQA-TMS-012 |
|
Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber
Description: 1 inch wide x 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyester Product: Cured Self-Fusing Silicone RubberCross-Section:..
|
|||
| Thickness | 1020 microns | 40.0 mil | |
|
3M Scotchkote™ 165HB Urethane Coating
3M Scotchkote Urethane Coating 165HB is a two component 100% solids urethane coating used for the internal and external protection of steel and concrete pipes, tanks, and vessels. It can be used in ..
|
|||
| Thickness | 1020 microns | 40.0 mil | Side 2; Arlon SQA-TMS-003 |
|
Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma..
|
|||