| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 81.3 microns | 3.20 mil | PTFE Coated Fiberglass, Substrate |
|
Arlon R36772R008 0.008" (0.203 mm) Fully Cured, Unsupported, Silicone Rubber with Fiberglass Substrate
(
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material ..
|
|||
| Thickness | 81.3 microns | 3.20 mil | |
|
Hexcel® HexForce™ 1620 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
|
|||
| Thickness | 81.3 microns | 3.20 mil | |
|
Hexcel® HexForce™ 112 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Total |
|
3M 1170 EMI Shielding Tape
3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 7000FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 7014FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 7779 Polypropylene Label Material
3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Backside Adhesive |
|
3M 9456 Double Coated Tapes with Adhesive 340
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 9459W Laminating Adhesive For Label Component Systems
3M™ Adhesive Transfer Tape 9459W is a high Performance 300 Adhesive with 55 lb Densified Paper Kraft Paper Liner. 1.5 mil Thick with 3.2 mil LinerFeatures:Bond high and low surface energy plastics,..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 9737 Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 9738R Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Facestock |
|
3M PS191 White Yupo™ TIS Label Products
3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Tape |
|
3M Scotch Pad™ 8325 Custom Carry Handle
3M™ Carry Handle 8325 is made of durable plastic strips with adhesive at each end. 3M ScotchPad Carry Handle 8325 is available with custom printed or colored carry portion materials. It is easy to ..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Release Liner |
|
3M XT2105-AGT Hi-Tack Adhesive Transfer Tape
3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Backing; ASTM D3752 |
|
3M 5451 PTFE Glass Cloth Tape
3M™ PTFE Glass Cloth Tape 5451 has a silicone adhesive which provides a high temperature release surface for protection and insulation.Information provided by 3M
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 7011FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 7604FP Primalyn™ White Vinyl Label Material
3M™ Primalyn™ White Vinyl Label Material 7604FP is a flexible vinyl providing excellent squeeze bottle performance with consistent printability. This material utilizes 3M™ Adhesive 300, which has..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 7881 Computer-Imprintable Polyester Label Material
Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Facestock |
|
3M PS190 White Yupo™ TIS Label Products
3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Facestock |
|
3M PS442 White Yupo™ EDP Label Product
3M™ White Yupo™ EDP Label Product PS442 is a matte white polypropylene material that offers excellent durability. This label product utilizes 3M™ Adhesive P1110, which is a general purpose perman..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 7840 Laser Toner Printable Polyester Label Material
3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Total; ASTM D3752 |
|
3M 8992L Polyester Tape
3M™ Polyester Tape 8992L is a dark green polyester tape with silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and ba..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Caliper |
|
3M 9593 Double Coated Tapes with Adhesive 350
3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a ..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 9626 Adhesive Transfer Tape with Quick Bonding Adhesive 360
3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai..
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner Caliper |
|
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
|
|||
| Thickness | 81.3 microns | 3.20 mil | Liner |
|
3M 9737R Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
|
|||