| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 86.4 microns | 3.40 mil | Nominal |
|
DuPont™ Nomex® 414 Paper, 3.4 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
|
|||
| Thickness | 86.4 microns | 3.40 mil | |
|
ExxonMobil Label-Lyte® 85 LP-200M Mirror Finish, Metallized, White Opaque OPP for Water-based Patch Label Applications
White, polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. It has an anti-static, "mirror finish" metallized print surface that is coro..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Backing; ASTM D3652 |
|
3M 363L Specialty Foil Tape
Linered version of 363Information provided by 3M
|
|||
| Thickness | 86.4 microns | 3.40 mil | ASTM D3652 |
|
3M 7300 Masking Film
3M™ 7300 Series Masking Film is a high performance, high temperature wide area masking film that is soft flexing for good drape and conformability.Information provided by 3M
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM010 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM027 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM030 Indoor UL Recognized Clear Polyester Label Products
on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM037 Indoor UL Recognized Clear Polyester Label Products
on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM090 Indoor UL Recognized Matte Silver Polyester Label Product
3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM110 Indoor UL Recognized Brushed Silver Polyester Label Products
3M™ Indoor UL Recognized Brushed Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utili..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM120 Indoor UL Recognized White Polyester Label Products
3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM157 Indoor UL Recognized Computer Imprintable Silver Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FP024900 White Polypropylene Label Products
3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FP100 Clear Polypropylene Label Product
3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FV090 Soft Translucent Vinyl Label Products
3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FV1220 Removable Vinyl Label Products
3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FV517 Semi-Rigid Vinyl Label Product
3M™ Semi-Rigid Vinyl Label Products are semi-rigid white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1410, which is a general purpose..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M PS197 White Yupo™ TIS Label Products
3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Facestock |
|
3M 7901 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Facestock |
|
3M 7904 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FM057 Indoor UL Recognized Brite Silver Polyester Label Products
3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FV030 Indoor UL Recognized White Vinyl Label Products
3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M PS190 White Yupo™ TIS Label Products
3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M PS472 White Yupo™ EDP Label Product
3M™ White Yupo™ EDP Label Products PS470 and PS472 are matte white opaque polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesiv..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Backing; ASTM D3652 |
|
3M 363 Specialty Foil Tape
Aluminum foil/glass cloth. Highest temperature metal foil tape.Information provided by 3M
|
|||
| Thickness | 86.4 microns | 3.40 mil | Facestock |
|
3M 7902 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Facestock |
|
3M 7906 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FV01460 Soft Clear Vinyl Label Products
3M™ Soft Clear Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Liner |
|
3M FV037 Indoor UL Recognized White Vinyl Label Products
3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,..
|
|||
| Thickness | 86.4 microns | 3.40 mil | Facestock |
|
3M FV038 Indoor UL Recognized White Vinyl Label Products
3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,..
|
|||