Polymer Property : Water Vapor Transmission = 35.0 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F127 PA6
Low/Medium Viscosity, Film Extrusion
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F130 PA6
Film Extrusion, Medium Viscosity
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F130-C PA6
Film Extrusion, Medium Viscosity, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F132 PA6
Film Extrusion, High Viscosity
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F132-E1 PA6
Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F132-E2 PA6
High Viscosity, Nucleated, Lubricated, Film Extrusion
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F136-C PA6
Film Extrusion, Very High Viscosity, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F136-C1 PA6
Very High Viscosity, Film Extrusion, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F136-E1 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F136-E2 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., Film; DIS 15106-1/-3
DSM Akulon® XP32-E1 PA6
Film Extrusion, Medium Viscosity, Lubricated, Nucleated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., Film; DIS 15106-1/-3
DSM Akulon® XP36-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., Film; DIS 15106-1/-3
DSM Akulon® XP32-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Water Vapor Transmission 35.0 g/m²/day

@Temperature 23.0 °C
2.25 g/100 in²/day

@Temperature 73.4 °F
at 85% r.h., Film; DIS 15106-1/-3
DSM Akulon® XP36-E1 PA6
Film Extrusion, Medium Viscosity, Nucleated, Lubricated
Water Vapor Transmission 35.0 g/m²/day
2.25 g/100 in²/day
Average value: 35.0 g/m²/day Grade Count:16
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..