| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ Dipolymer, 35% Carbon Black Filled
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb.
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5610Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5621Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5623Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5640Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5641Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5660Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2110Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Viscosity ..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2174 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested ..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5622Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FE-5642Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2122 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good flow, release and hot tear for c..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2123 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent hot tear and compression se..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2144 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Higher viscosity version of FC-2123. ..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2152 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved hot tear over FC-2176. Sugg..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good ..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2177 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Slower cure rate and high tear streng..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2181 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Combines high elongation with excelle..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FLS-2530 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. High fluorine dipolymer with improved f..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2120 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for difficult extrusions. ..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2182 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for autoclave curing. Used..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2145 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2261Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FT-2481 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2211 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FC-2260 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl ..
|
|||
| Oxygen Transmission | 98.0 cc-mm/m²-24hr-atm | 249 cc-mil/100 in²-24hr-atm | |
|
3M Dyneon™ Fluorel™ FG-5690Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia..
|
|||