Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brookfield Viscosity = 1000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Brookfield Viscosity 1000 cP
1000 cP
70% solids dispersed using a Brookfield #3 spindle at 100 rpm
Old Hickory M&M Clays, Inc. Wilco-UPF Kaolin Clay
Wilco UPF is finer grained kaolin and can be employed in a ceramic formulation where higher permeability type kaolin is not required. It has excellent suspension qualities and lends good film streng..
Brookfield Viscosity 1000 cP
1000 cP
60 rpm; ISO 1652
Polimeri Europa Intex® 132 Styrene - Butadiene Copolymer
Intex® 132 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain an..
Brookfield Viscosity 1000 cP
1000 cP
60 rpm; ISO 1652
Polimeri Europa Intex® 2720 Styrene - Butadiene Copolymer
Intex® 2720 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain a..
Brookfield Viscosity 1000 cP
1000 cP
60 rpm; ISO 1652
Polimeri Europa Intex® 2740 Styrene - Butadiene Copolymer
Intex® 2740 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain a..
Brookfield Viscosity 1000 cP
1000 cP
RVT Spindle 3 @ 20 rpm
Palm Labs Adhesives TURBO-LOCK SERIES 10 Anaerobic Thread Locking Compound
TURBO-LOCK SERIES 10 is a removable, PURPLE, fast curing, low strength, anaerobic thread-locking compound for bonding and sealing small screw threads. It is highly resistance to heat, vibrations, wa..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
#20/200
Mallard Creek Polymers Rovene® 5499 Styrene-Butadiene Emulsion
Rovene® 5499 is a styrene-butadiene emulsion that was developed as an ink vehicle for TPO based wall coverings. More specifically it can be formulated for metallic ink vehicles. Rovene® 5499 p..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
#20/200
Mallard Creek Polymers Rovene® 6112 Resin Supported Emulsion
Rovene® 6112 is a hard, film forming, low glycol ether and VOC vehicle with a moderately low glass transition temperature for flexographic and gravure inks and overprint varnishes. Rovene® 611..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
#20/200
Mallard Creek Polymers Rovene® 6115 Resin Supported Emulsion
Rovene® 6115 is a hard, non-film forming vehicle that is neutralized with sodium hydroxide for flexographic and gravure inks and overprint varnishes primarily for use on paper and paperboard subs..
Brookfield Viscosity 1000 - 5000 cP
1000 - 5000 cP
DOP 60phr; ASTM D1824
LG Chemical PB1752 PVC
General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for sk..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Michelman® Hydrosize® U1-03 Phenoxy modified polyurethane dispersion
Description: Phenoxy modified polyurethane dispersionUsage: Hydrosize® U1-03 is designed to be a fiber sizing coating with excellent adhesion and abrasion resistanceInformation provided by Michel..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Michelman® Michem® Emulsion 28640 Cationic polypropylene emulsion
Description: Cationic polypropylene emulsionUsage: Michem® Emulsion 28640 is a used as a binder and substrate coating for fibers and composites.We serve many markets through Michem® Emulsion, ..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Michelman® Michem® Emulsion 91735 Nonionic polypropylene emulsion
Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 91735 is a sizing polymer for fiberglass and other fibers used to reinforce polypropylene.We serve many markets through MichemÂ..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Michelman® Michem® Emulsion 91840 Nonionic HD polyethylene / paraffin wax emulsion
Description: Nonionic HD polyethylene / paraffin wax emulsionUsage: Michem® Emulsion 91840 is a wax emulsion that provides superior rub resistance and gloss when used as an additive in overprint ..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Michelman® Michem® Lube 270R Anionic paraffin/polyethylene wax emulsion
Description: Anionic paraffin/polyethylene wax emulsionUsage: Michem® Lube 270R is an additive which provides excellent water resistance in paint and coating formulations. This product is useful ..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Michelman® Michem® Shield 422 Anionic dispersion of polyethylene wax
Description: Anionic dispersion of polyethylene waxUsage: Michem® Shield 422 provides superior rub resistance in graphic arts applications.Information provided by Michelman®
Brookfield Viscosity 1000 cP
1000 cP
Measured on 25% mass solution in toluene at 25°C; BMS 0380
Kraton® D1152 E (SBS) Liner Block Copolymer
Description: Kraton D1152 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
Brookfield Viscosity 1000 cP
1000 cP
25% Toluene Solution at 25°C; KM 06
Kraton® D1160 E (SIS) Linear Triblock Copolymer
Description: Kraton D1160 E is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from Europe in the physical form identified: D1160 ES ..
Brookfield Viscosity 1000 cP

@Temperature 25.0 °C
1000 cP

@Temperature 77.0 °F
Toluene solution. Neat polymer concentration, 25%w.
Kraton® D4141 (SBS) Linear Block Copolymer
(SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact ..
Brookfield Viscosity 1000 - 1900 cP

@Temperature 25.0 °C
1000 - 1900 cP

@Temperature 77.0 °F
20% Toluene solution; KM 06
Kraton® G1650 E (SEBS) Linear Block Copolymer
Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms i..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Michelman® Hydrosize® U1-01 Nonionic polyurethane dispersion
Description: Nonionic polyurethane dispersionUsage: Hydrosize® U1-01 is a sizing for chopped glass and carbon fiber with excellent adhesion and good color and pH stability.Application data: Soft,..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
Spindle # 3, rpm 60
Michelman® Michem® Emulsion 54255 Multi-functional epoxy dispersion
Description: Multi-functional epoxy dispersionUsage: Michem® Emulsion 54255 is a modified multi-functional epoxy dispersion which exhibits exceptional flexibility and toughness. It can be used fo..
Brookfield Viscosity 1000 - 1400 cP
1000 - 1400 cP
Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® 46-10/12 Polyester based TPU
Pearlstick 46-10/12 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a high thermoplasticity level. Solubility:..
Brookfield Viscosity <= 1000 cP
<= 1000 cP
#3 SP, 12 rpm; RP-0596
Solvay DERMALCARE® MAP L 213 K Surfactant
Description: High purity Potassium Monoalkyl Phosphate based off patented Rhodia process. A pre-neutralized MAP solution, MAP-L-213/K provides a dense creamy lather and is extremely mild to skin. In..
Brookfield Viscosity 1000 - 1600 cP

@Temperature 25.0 °C
1000 - 1600 cP

@Temperature 77.0 °F
10% solids aqueous solution, #3 spindle, Model LVF, 60 rpm
DuPont Elvanol® 85-91 Polyvinyl Alcohol Specialty and Adhesive Grade
Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late..
Brookfield Viscosity 1000 - 1400 cP

@Temperature 25.0 °C
1000 - 1400 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 203 Special Laminate
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 203: Polyester resin..
Brookfield Viscosity 1000 - 3000 cP
1000 - 3000 cP
Part A, CP#52 @ 100 rpm
3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigg..
Brookfield Viscosity 1000 - 3000 cP
1000 - 3000 cP
Part A, CP#52 @ 100 rpm
3M Scotch-Weld™ DP600NS Concrete Repair and Self-Leveling
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600NS is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a tri..
Brookfield Viscosity 1000 - 3000 cP
1000 - 3000 cP
Part A, CP #52 @ 100 rpm
3M Scotch-Weld™ DP601 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Brookfield Viscosity 1000 cP
1000 cP
Catalyst
BCC Products BC 9040 T Silicone RTV Rubber
BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high..
Brookfield Viscosity 1000 - 3000 cP
1000 - 3000 cP
RVT #3 sp @ 20 rpm
3M Scotch-Weld™ RT3500B Rubber-Toughened Instant Adhesive
3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon..
Copyright © lookpolymers.com All Rights Reserved