Polymer Property : Brookfield Viscosity = 6000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Brookfield Viscosity 6000 - 12000 cP
6000 - 12000 cP
RVT (15% in MEK); MQSA 40 A
Lubrizol Advanced Materials PEARLBOND® 110 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® 110 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a low thermoplasticity level.Applications: P..
Brookfield Viscosity 6000 - 14000 cP
6000 - 14000 cP
Fusor 2002; LVT, Spindle #4 @ 30rpm
Lord Adhesives Fusor® 2001 / 2002 Urethane Adhesive
Fusor® 2001/2002 is a two-part urethane adhesive system used to bond fiberglass reinforced plastics, sheet molded compound, and bulk molded compound to themselves as well as to primed metals.All ..
Brookfield Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
Spindle CP40 @ 5rpm
Lord Adhesives Thermosetâ„¢ ME-525 Underfill Encapsulant
LORD Thermosetâ„¢ ME-525 encapsulant is a high purity, semiconductor grade epoxy underfill product developed for the encapsulation of flip chip devices. It is formulated to reduce warpage and wit..
Brookfield Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
Loctite® 3091 Light Cure Acrylic Adhesive
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..
Brookfield Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
Loctite® 3100 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Brookfield Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
Loctite® 3101 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Brookfield Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
Loctite® 3335 Epoxy Light Cure Adhesive
Epoxy Light Cure AdhesivesLoctite® 3335 Epoxy Light Cure AdhesiveA one-part, medium viscosity, cationic epoxy. Excellent for surface cure - no oxygen inhibition. Low outgassing, very good high temp..
Brookfield Viscosity 6000 cP
6000 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Formosa Plastics Formolon® 10 PVC
PVC Homopolymer Dispersion Resin F-10 is a medium molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Plastisol prepared using F-10 exhibit low paste viscosity as..
Brookfield Viscosity 6000 - 8000 cP
6000 - 8000 cP
RVT #4 sp @ 20 rpm
3M Scotch-Weld™ TL77 Threadlocker Anaerobic Adhesive
3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening..
Brookfield Viscosity 6000 cP

@Temperature 191 °C
6000 cP

@Temperature 375 °F
3M Scotch-Weld™ 3764 Hot Melt Adhesive
Bonds variety of plastics including polycarbonate, polyethylene, and polypropylene and Flexible at low temperaturesInformation provided by 3M
Brookfield Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
Mixed
Loctite® Durabond® M-31CL Epoxy Adhesive
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..