| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
|
Imerys DB-Floatâ„¢ Kaolin
Information provided by Imerys
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.1% retained |
|
Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin
KT 90A-1 is a Hydraetd Aluminum Silicate. It is a high surface area, fine particle size clay that is well suited for use as an econoMical filler.Information provided by Imerys
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.25% max retained |
|
Imerys Mercapâ„¢ 100 Kaolin
Information provided by Imerys
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | less than 0.01% retained |
|
Imerys Minsparâ„¢ 7 Ground Feldspar
Minsparâ„¢ 7 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 7 is easily dispersed to a high Hegman grind to produce coatings with hig..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.8% Retained |
|
KaMin FIBEREX®
FIBEREX® is an economical fiber extender for liner board and/or newsprint. Industry: PAPER & PACKAGINGUses: Coated Recycled Board, Coated Natural Kraft, LinerboardInformation provided by KaMin L..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
|
KaMin Hydraprint® Kaolin Clay - Filler
Hydraprint® kaolin clay is a standard delaminated filler for paper applications. Industry: PAPER & PACKAGINGUses: Coated 1S Label, Coated Bleached Board, Coated Recycled Board, Coated Natural Kra..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
|
KaMin KaMin® HG Kaolin Clay - Waterwashed
KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | Powder |
|
Lucas-Milhaupt Lucanex 721 Active Metal Brazing
Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.01% Retained |
|
KaMin Nylok® 171 Kaolin Clay - Surface Treated
Amino silane treated calcined kaolin that reinforces polyamide resin systems.Industry: Rubber & PlasticUses: Non-Black Rubber, Nylon, Thermoset, ThermoplasticInformation provided by KaMin LLC.
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
|
Silberline 4-Allâ„¢ LEP 20051
The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
|
Silberline A-6571FG
A-6571FG is a standard polished grade; class A, fine leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
|
Silberline Extra Fine "T"
Extra Fine "T" is a standard polished grade; class "A", fine, leafing aluminum pigment carried in mineral spirits.Applications: Trade & Maintenance
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
|
Silberline Lansford 243 Standard Series
Lansford 243 - is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This is a very economical grade with cornflake geometry and wide particle size distrib..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
|
Silberline SilBerCote® PC 3101X
SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
|
Silberline SilBerCote® PC 8153X
SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
|
Silberline Sparkle Silver® 5245-AR
Sparkle Silver® 5245-AR is a medium, non-leafing aluminum pigment. It provides a bright, white, clean face tone with exceptionally dark flop effect. It has narrow particle size distribution. Clos..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
|
Silberline Sparkle Silver® 5251-AR
Sparkle Silver® 5251-AR is a medium particle size, bright, non-leafing aluminum pigment with a smooth patina. It provides exceptional brightness and is acid resistant.Applications: Automotive
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
|
Silberline Sparkle Silver® Premier 454
Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
|
Silberline Sparkle Silver® Premier 556
Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
|
Silberline Sparkle Silver® Premier 751
Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 2% retained |
|
Silberline Stamford "Q" Standard Series
Stamford Q - is a medium size, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This is an economical grade with cornflake geometry and wide particle size distri..
|
|||
| Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
|
Silberline Tufflake® 2722
Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 100% passes |
|
Excalibar ExBar™ W 4 Barite BaSO4 Powder
ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, ..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 84% Passes |
|
Excalibar ExCal® CW 200 Calcium Carbonate CaCO3 Powder
ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 97% Passes |
|
Excalibar ExCal® CW 325 Calcium Carbonate CaCO3 Powder
ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.1% retained |
|
CIMBAR CIMTUFF® 9107 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 75 - 85% passing, dry |
|
CIMBAR RMF 75 Recycled Mineral Filler
Cimbar RMF is a locally sourced, third-party certified recycled filler containing 90% Post-Consumer materials. They are a clean, safe, environmentally-friendly alternative for use in various polyme..
|
|||
| Particle Mesh Size | 325 Mesh | 325 Mesh | 100% passing |
|
CIMBAR UltraMag & UltraMag ST 3 Magnesium Hydroxide Powder
UltraMag is a naturally ground, white, high-purity Magnesium Hydroxide suitable for a wide range of applications including water treatment slurries, plastics, rubber and flame-retardant/smoke suppre..
|
|||