| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Mesh Size | 60 - 80 Mesh | 60 - 80 Mesh | US Sieve |
|
Potters Industries A-Series P-0100 Soda-Lime Silica Technical Quality Solid Glass Spheres
Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil..
|
|||
| Particle Mesh Size | 60 - 100 Mesh | 60 - 100 Mesh | |
|
Potters Industries Spheriglass® 1922 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 5% max retained; SABIC (PVC 003) |
|
SABIC PVC 59S Suspension Polyvinyl Chloride for Rigid Products
Product Description: PVC 59S is a free flowing vinyl chloride homopolymer resin having low molecular weight. It is manufactured by suspension polymerization.Characteristics: PVC 59S has the follo..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 15% max retained; SABIC (PVC 003) |
|
SABIC PVC 67S Suspension Polyvinyl Chloride for Rigid Extruded Products
Product Description: PVC 67S is a free flowing vinyl chloride homopolymer resin having medium molecular weight. It is manufactured by suspension polymerization.Characteristics: PVC 67S has the fo..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 15% max retained; SABIC (PVC 003) |
|
SABIC PVC 70S Suspension Polyvinyl Chloride for Flexible Products
Product Description: PVC 70S is a free flowing vinyl chloride homopolymer resin having a high molecular weight. It is manufactured by suspension polymerization.Characteristics: PVC 70S has the fo..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 5% Retention; PVCH/QCD/3514 |
|
Reliance Industries 57-01 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications: Rigid injection.
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 5% Retention; PVCH/QCD/3514 |
|
Reliance Industries 60-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusionRigid injectionRigid calenderingCan be used:Blow molding
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 10% Retention; PVCH/QCD/3514 |
|
Reliance Industries 67-01 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusion.Can be used:rigid injection.
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 10% Retention; PVCH/QCD/3514 |
|
Reliance Industries 67-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications: Recommended:Flexible extrusionFlexible injectionFlexible calenderingCan be used:Rigid injectionRigid extrusion
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 5% Retention; PVCH/QCD/3514 |
|
Reliance Industries 57-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications: Rigid injectionRigid extrusionRigid calenderingblow molding
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
|
Chevron Phillips Ryton® PR37 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
|
Chevron Phillips Ryton® PR26 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
|
Chevron Phillips Ryton® PR25 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
|
Chevron Phillips Ryton® PR27 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
|
Chevron Phillips Ryton® PR34 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
|
Chevron Phillips Ryton® PR35 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
|
Chevron Phillips Ryton® PR06 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 75 wt% Passing |
|
Chevron Phillips Ryton® PR39 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
|
Chevron Phillips Ryton® P-4 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
|
Solvay Specialty Polymers Ryton® P-6 Polyphenylene Sulfide Coating Resin
(Unverified Data**)
Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line.
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 0.05% retained |
|
Imerys Kaolexâ„¢ FG Kaolin
Kaolex FG is a air floated Hydrated Aluminum Silicate. Its low surface area makes it a good choice for fiberglass manufacturing.Information provided by Imerys
|
|||
| Particle Mesh Size | 60 - 100 Mesh | 60 - 100 Mesh | 0.1623 |
|
Gromax Standard GB9567-97
China NInformation provided by Gromax Enterprises Corp.
|
|||
| Particle Mesh Size | 60 - 100 Mesh | 60 - 100 Mesh | 0.1973 |
|
Gromax Standard GB9567-97
China SInformation provided by Gromax Enterprises Corp.
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | Opening 1700µm; ASTM E11 |
|
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS
Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th..
|
|||
| Particle Mesh Size | 60 - 80 Mesh | 60 - 80 Mesh | |
|
Beijing Evergrow Resources ACFP-60 Activated Carbon Fiber Powder
Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 10% Retention; PVCH/QCD/3514 |
|
Reliance Industries 70-21 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications:Can be used:Flexible extrusionFlexible injectionFlexible calendering
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 90 wt% Passing |
|
Chevron Phillips Ryton® PR33 Polyphenylene Sulfide Resin
(discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 95 wt% Passing |
|
Solvay Specialty Polymers Ryton® PR11 Polyphenylene Sulfide Resin
(Unverified Data**)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 99.5 wt% Passing |
|
Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide Coating Resin
(Unverified Data**)
Characteristics: High temperatureNon-stickCorrosion resistantApplications: CoatingsInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line.
|
|||
| Particle Mesh Size | 60 Mesh | 60 Mesh | 95 wt% Passing |
|
Chevron Phillips Ryton® PR11 Polyphenylene Sulfide Coating Resin
(Unverified Data**)
Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line.
|
|||