Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Tension = 56 dynes/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D5946
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D5946
Honeywell Capran® Emblem™ 1200M Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ 1200M is a 0.48 mil (12 micron) biaxially oriented nylon 6 film with a polymeric coating which provides enhanced adhesion to a variety of inks, coatings, and adh..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film
Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ M-OPA (0.60 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ M-OPA (0.75 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ M-OPA (1.0 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ OBS Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Barrer is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier through a bro..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ OEB (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Extra Barrier is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of ..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ OEB (1.0 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Extra Barrier is a 1.00 (25micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relat..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ OMBS (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Medium Barrier is a 0.60 mil (15 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ OMBS (1.00 mil) Monoaxially Oriented, Co-Extruded Nylon 6-Based Clear Film
Description: Oxyshieldâ„¢ Oriented Medium Barrier is a 1.00 mil (25 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 0.6 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of ..
Surface Tension >= 56 dynes/cm
>= 56 dynes/cm
treated side; ASTM D2578
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 1.0 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of ..
Copyright © lookpolymers.com All Rights Reserved