| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bead Size | 0.800 - 1.60 mm | 0.0315 - 0.0630 in | |
|
IRPC Polimaxx Pentfoam 291L Expandable Polystyrene
General: Pentfoam 291L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application..
|
|||
| Bead Size | 0.800 - 1.40 mm | 0.0315 - 0.0551 in | |
|
BASF Neopor® 2300 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
|
|||
| Bead Size | 0.800 - 1.30 mm | 0.0315 - 0.0512 in | |
|
Ineos Nova W441A Expandable Polystyrene
A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for..
|
|||