| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bead Size | 0.700 - 1.20 mm | 0.0276 - 0.0472 in | |
|
NOVA Chemicals Dytherm® 150F Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
NOVA Chemicals Dytherm® 150R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
NOVA Chemicals Dytherm® 250R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
NOVA Chemicals Dytherm® 350R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
Ineos Nova Styrocell® M544C Expandable Polystyrene
A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell is..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
Ineos Nova T523C Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for medium density foam.Applications: This grade is used mainly ..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
Ineos Nova T543B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for medium density foam.Applications: This grade is used mainly ..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
Iran Petrochemical (PCC) TPC - 323 FC Expandable Polystyrene
TPC - 323 FCApplications: faster cycling shape molding with wall thickness >10mm, medium to high density blocksInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
BASF Styropor® F 315-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
BASF Styropor® F 395 -N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat..
|
|||
| Bead Size | 0.700 - 0.900 mm | 0.0276 - 0.0354 in | |
|
BASF Styropor® P 326 M Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded parts with very good mechanical ..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
BASF Peripor® 300 Expandable Polystyrene
Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low ..
|
|||
| Bead Size | 0.700 - 0.900 mm | 0.0276 - 0.0354 in | |
|
BASF Styropor® P 326 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS..
|
|||
| Bead Size | 0.700 - 0.900 mm | 0.0276 - 0.0354 in | |
|
BASF Styropor® P 326 Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS..
|
|||
| Bead Size | 0.700 - 1.40 mm | 0.0276 - 0.0551 in | > 95% in this range per Berre Laboratory Analytical Methods 0492 |
|
Ineos Nova W441A Expandable Polystyrene
A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for..
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
Iran Petrochemical (PCC) TPC - 321 HS Expandable Polystyrene
TPC - 321 HSApplications: shape molding with wall thickness > 10 mm, medium to high density blocksInformation provided by Iran Petrochemical Commercial Co.
|
|||
| Bead Size | 0.700 - 1.00 mm | 0.0276 - 0.0394 in | |
|
Iran Petrochemical (PCC) TPC - 326 WP Expandable Polystyrene
TPC - 326 WPApplications: low water absorption, longer cycling shape molding with wall thickness >10 mmInformation provided by Iran Petrochemical Commercial Co.
|
|||