Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bead Size = 0.900 mm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Bead Size 0.900 - 1.40 mm
0.0354 - 0.0551 in
SABIC EPS 650FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 650FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Bead Size 0.900 - 1.40 mm
0.0354 - 0.0551 in
SABIC EPS 652 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 652 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
Bead Size 0.900 - 1.60 mm
0.0354 - 0.0630 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 140R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.900 - 1.60 mm
0.0354 - 0.0630 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 240R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.900 - 1.60 mm
0.0354 - 0.0630 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 340R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.900 - 1.30 mm
0.0354 - 0.0512 in
BASF Neopor® 5300 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Bead Size 0.900 - 1.30 mm
0.0354 - 0.0512 in
BASF Neopor® 5300 Plus Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Bead Size 0.900 - 1.30 mm
0.0354 - 0.0512 in
BASF Styropor® P 226 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Blocks with very short cycle times.Info..
Copyright © lookpolymers.com All Rights Reserved