Physical Properties Metric English Comments
Bead Size 1.00 - 1.30 mm
0.0394 - 0.0512 in
Ineos Nova T443B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..
Bead Size 0.900 - 1.30 mm
0.0354 - 0.0512 in
BASF Neopor® 5300 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Bead Size 0.900 - 1.30 mm
0.0354 - 0.0512 in
BASF Neopor® 5300 Plus Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Bead Size 1.02 - 1.30 mm
0.0402 - 0.0512 in
BASF Styropor® KF 262M EPS
Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with..
Bead Size 0.900 - 1.30 mm
0.0354 - 0.0512 in
BASF Styropor® P 226 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Blocks with very short cycle times.Info..
Bead Size 0.800 - 1.30 mm
0.0315 - 0.0512 in
Ineos Nova W441A Expandable Polystyrene