Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bead Size = 2.50 mm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Bead Size 1.20 - 2.50 mm
0.0472 - 0.0984 in
SABIC EPS 760FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 760FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Bead Size 1.20 - 2.50 mm
0.0472 - 0.0984 in
SABIC EPS 763 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 763 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
Bead Size 1.80 - 2.50 mm
0.0709 - 0.0984 in
Iran Petrochemical (PCC) TPC - 121 HS Expandable Polystyrene
TPC - 121 HSApplication: low density blocksInformation provided by Iran Petrochemical Commercial Co.
Bead Size 1.25 - 2.50 mm
0.0492 - 0.0984 in
IRPC Polimaxx Pentfoam 193L Expandable Polystyrene
General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application..
Bead Size 1.25 - 2.50 mm
0.0492 - 0.0984 in
IRPC Polimaxx Pentfoam 241F Expandable Polystyrene
General: Pentfoam 241F is a regular grade expandable polystyrene containing pentane as blowing agentApplications: Pentfoam 241F is particularly well suited for the manufacture of eps insulation boar..
Bead Size 1.40 - 2.50 mm
0.0551 - 0.0984 in
BASF Neopor® 2200 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Copyright © lookpolymers.com All Rights Reserved